Alloy Digest (2013) 62 (1): SS-1132.
Published: 01 January 2013
... DMV 800 is a heat-resisting austenitic stainless steel with 33 Cr. The alloy has good high-temperature properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion...
Journal Articles
Alloy Digest (2011) 60 (11): Ni-692.
Published: 01 November 2011
... DMV 617 Modified is a superheater boiler tubing grade with strength and corrosion resistance for ultra supercritical boilers. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes...
Journal Articles
Alloy Digest (2015) 64 (2): Ni-721.
Published: 01 February 2015
... (1.9) Creep rupture strength, 100,000 h min, MPa (ksi) 600 °C (112 °F) 97 (14.1) 700 °C (1292 °F) 42 (6.1) 800 °C (1472 °F) 17 (2.5) 850 °C (1562 °F) 9 (1.3) 900 °C (1652 °F) 7 (1.0) DMV 600/600H (Nickel Alloy) Filing Code: Ni-721 Nickel :: February 2015 Materials Park, Ohio 44073-0002 :: 440.338.5151...
Journal Articles
Alloy Digest (2000) 49 (6): SS-795.
Published: 01 June 2000
...: DMV Stainless USA, Inc. Houston, TX 77041 (713) 466 7278 (713) 466 3769 (fax) ISSN: 002-614X SS-795B Fig. 1 Isocorrosion chart for 0.1 mm/y (4 mpy) in sulfuric acid Fig. 3 Pitting potential as a function of tempera- ture in 0.5 M NaCl, polarization rate 250 mV/h Applied potential, mV (SCE) 1200 800...
Journal Articles
Alloy Digest (2009) 58 (12): SS-1048.
Published: 01 December 2009
... DMV 928 is a nickel-base alloy with high alloying elements of chromium, molybdenum, and copper for excellent corrosion resistance in reducing and oxidizing media. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (2008) 57 (6): SS-1014.
Published: 01 June 2008
... be avoided or eliminated. Corrosion Resistance: DMV 316 LUG exhibits excellent resistance to oxidation and a low rate of scaling in an air atmosphere. This alloy is barely susceptible to precipitation of chromium carbides in grain boundaries when exposed to temperatures in the range of 430 820 °C (800 1500...
Journal Articles
Alloy Digest (2009) 58 (1): SS-1027.
Published: 01 January 2009
... DMV 310 N is a special modification of 310, an austenitic stainless steel, by additions of both nitrogen and niobium. This addition results in increased elevated-temperature strength and creep resistance. The alloy has potential in advanced boilers with high steam temperatures. This datasheet...
Journal Articles
Alloy Digest (2009) 58 (11): SS-1047.
Published: 01 November 2009
... DMV 931 is an alloy for general and chloride corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (2008) 57 (5): SS-1013.
Published: 01 May 2008
... to temperatures in the range of 430 820 °C (800 1500 °F). Such sensitized steels are subject to intergranular corrosion and/or intergranular stress-corrosion cracking (SCC) when exposed to aggressive environments. DMV 25.22.2 is less susceptible to SCC in halide environments than other austenitic stainless steel...
Journal Articles
Alloy Digest (2012) 61 (12): Ni-704.
Published: 01 December 2012
... DMV 825 is a nickel alloy with 21% Cr. The alloy has a balanced composition for use in both oxidizing and reducing conditions. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1994) 43 (7): SS-569.
Published: 01 July 1994
... S.p.A. 24044 Dalmine (035) 563381 DMV Stainless Houston, TX 77041 (7 13) 466-7278 C Temperalure C ( F) :2% II Boiling in\ CuNC 100 -. I . L (210) 60 (140) (85) 1 2 3 4 HCI, weight - % (C) Isocorrosion diagram in hydrochloric add. The curves repra ssnt a corrosion rata of 0.1 mm/year (4 mpy) in stagnant...