Alloy Digest (2009) 58 (1): SS-1027.
Published: 01 January 2009
... DMV 310 N is a special modification of 310, an austenitic stainless steel, by additions of both nitrogen and niobium. This addition results in increased elevated-temperature strength and creep resistance. The alloy has potential in advanced boilers with high steam temperatures. This datasheet...
Journal Articles
Alloy Digest (2000) 49 (6): SS-795.
Published: 01 June 2000
... in., % 450 min 65 min 680 880 99 128 25 Table 2 Stress-Corrosion Cracking Tests Steel grade Test piece/method DMV 22.5, annealed 316L, annealed In MgCl2, 45%, boiling, 155 °C (310 °F) U-bent Rupture Rupture 4-point bent-beam test, stress before rupture, % of yield strength 100 50 C-ring test, stress before...