Alloy Digest (2008) 57 (5): SS-1013.
Published: 01 May 2008
... DMV 25.22.2 is a special low-carbon austenitic stainless steel. It has a very low ferrite content to resist corrosion in urea-related applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high...