1-7 of 7 Search Results for

DMV 22.5

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2000) 49 (6): SS-795.
Published: 01 June 2000
... DMV 22.5 is a ferritic-austenitic grade with very good resistance to stress-corrosion cracking (SCC), chlorides, fresh water, and high pressures. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (2000) 49 (5): SS-785.
Published: 01 May 2000
... Isocorrosion curve in phosphoric acid, 0.1mm/yr Stress corrosion cracking H2S 1 bar 120 100 80 60 40 20 0 316 L DMV 22.5 DMV 25.7 N 20 °C 60 °C Threshold stress which does not cause rupture in one month in NACE TM 01-77 solution Fig. 3 Stress corrosion cracking in H2S, 1 bar Stress corrosion cracking in...
Journal Articles
Alloy Digest (2013) 62 (1): SS-1132.
Published: 01 January 2013
... DMV 800 is a heat-resisting austenitic stainless steel with 33 Cr. The alloy has good high-temperature properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion...
Journal Articles
Alloy Digest (2008) 57 (11): SS-1022.
Published: 01 November 2008
... DMV 347 HFG is produced as seamless tubing suitable as a replacement for old reheater and superheater boiler tubes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature...
Journal Articles
Alloy Digest (2009) 58 (11): SS-1047.
Published: 01 November 2009
... DMV 931 is an alloy for general and chloride corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and...
Journal Articles
Alloy Digest (2011) 60 (11): Ni-692.
Published: 01 November 2011
... DMV 617 Modified is a superheater boiler tubing grade with strength and corrosion resistance for ultra supercritical boilers. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes...
Journal Articles
Alloy Digest (2008) 57 (5): SS-1013.
Published: 01 May 2008
... DMV 25.22.2 is a special low-carbon austenitic stainless steel. It has a very low ferrite content to resist corrosion in urea-related applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high...