Alloy Digest (2012) 61 (1): SA-641.
Published: 01 January 2012
... Dillidur 500V is a water hardened wear-resistant steel with surface hardness at room temperature of 470-530 HB. It has the highest wear resistance of the Dillidur steels. It is used in the production of transport systems, earth-moving plants, recycling plants, and stone crushers. This datasheet...
Journal Articles
Alloy Digest (2013) 62 (9): SA-681.
Published: 01 September 2013
... Dillidur 500V is a water hardened wear-resistant steel with surface hardness at room temperature of 310-370 HB. It has a high resistance to abrasion and impact wear in combination with good welding performance. This steel is used in the production of excavator buckets, stone crushers, and loading...