Alloy Digest (2011) 60 (9): SA-634.
Published: 01 September 2011
... Dillidur 325L is a wear resistant steel with a surface hardness at room temperature of 325 HB for 10 mm plate thickness. The material is easy to bend, hot work and machine. Due to its increased wear resistance, it is used to produce excavators, conveyors, and materials handling systems as well...