Alloy Digest (1976) 25 (12): TS-310.
Published: 01 December 1976
... DEWARD is an oil-hardening, non-deforming, manganese die steel that is characterized by uniformity, good machinability and satisfactory performance in service. Its composition permits a relatively low hardening temperature to give minimum distortion after heat treatment and little danger...