Alloy Digest (1989) 38 (11): P-12.
Published: 01 November 1989
... DERAKANE 470-36 and 470-45 resins combine corrosion resistance with superior retention of properties at high temperatures and oxidation resistance. They cure rapidly to give fast green strength and superior creep resistance. This datasheet provides information on composition, physical properties...