Alloy Digest (2011) 60 (4): Ni-689.
Published: 01 April 2011
...: Stellite Coatings. Producer or Source: Stellite Coatings Copyright © ASM International® 2011 2011 ASM International chemical composition DELORO 15 ALLOYS DELORO 21 ALLOYS DELORO 22 ALLOYS DELORO 25 ALLOYS hardness molds nickel powder physical properties powder metal products DATA...
Journal Articles
Alloy Digest (2021) 70 (11): Co-142.
Published: 01 November 2021
... Deloro Stellite 25 is a cobalt-chromium-tungsten-nickel alloy. This tungsten strengthened cobalt-chromium alloy is the cast version of the wrought cobalt-base alloy L605. Deloro Stellite 25 is resistant to wear, galling, and corrosion and retains this resistance at high temperatures. Its...
Journal Articles
Alloy Digest (2010) 59 (11): Ni-683.
Published: 01 November 2010
... Deloro 50 EXV is also called Deloro 53. It is a self-fluxing alloy for abrasion and corrosion resistance. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties as well as fracture toughness. It also includes information on wear...
Journal Articles
Alloy Digest (1993) 42 (2): Ni-422.
Published: 01 February 1993
... Elongation Strength in 1 inch Hot Hardness Ksi (MPa) percent Rockwell C 95 (656) 2 - - zi 79 (545) 3 25 - - 35 79(545-) 4 20 - - 31 62 (428) 7 82R, - - !JoRB Table 2 - ADHESIVE WEAR TEST DATA P/-M-O.1 cast - 0.1 Table 3 - ABRASIVE WEAR TEST DATA P/M- 17 cast - 35 Joining: DELORO alloys can be joined to other...
Journal Articles
Alloy Digest (1993) 42 (3): Ni-424.
Published: 01 March 1993
... 37 cast 95 (652) cl - 1400(760) P/M 70 (483) 25 cast 91(626) i - Table 2 - TRANSVERSE RUPTURE STRENGTH KS1 (MPA) P/M- 117 (807) cast - Table 3 - ABRASIVE WEAR TEST DATA P/M- cast - 0.06 Joining: DELORO alloys can be joined to other materials by brazing and/or wcld- hg. If he pans are to be bramd...
Journal Articles
Alloy Digest (1993) 42 (5): Ni-431.
Published: 01 May 1993
... DELORO 711 PM is a nickel-base alloy recommended for handling conditions of wear, erosion, heat and corrosion when impact is also a consideration. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1993) 42 (7): Ni-435.
Published: 01 July 1993
... DELORO 716 PM is a nickel-base alloy recommended for handling conditions of wear, erosion, heat and corrosion when impact is also a consideration. This datasheet provides information on composition, physical properties, and hardness. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (1968) 17 (6): Co-55.
Published: 01 June 1968
... DELORO STELLITE-100 is a hard and abrasion resistant alloy designed specifically for metal cutting purposes. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (1996) 45 (12): SS-662.
Published: 01 December 1996
... both corrosion and galling. This alloy relies on the formation of chromium-rich carbides during soliditication. It is the lowest in catbon of the TtistelJe Family. The alloy is recommended for valve services. Tristelle and Stellite are uademarks of stoody Deloro stellite. Inc. Chemical Composition, wt...
Journal Articles
Alloy Digest (1997) 46 (1): SS-668.
Published: 01 January 1997
.... Producer or source: Stoody Deloro Stellite Inc. Producer or Source: Stoody Deloro Stellite Inc. Copyright © ASM International® 1997 1997 ASM International chemical composition corrosion-resistant alloys fracture toughness hardness joinability physical properties TRISTELLE ALLOY TS-2...
Journal Articles
Alloy Digest (1997) 46 (2): SS-672.
Published: 01 February 1997
... or source: Stoody Deloro Stellite Inc. Producer or Source: Stoody Deloro Stellite Inc. Copyright © ASM International® 1997 1997 ASM International chemical composition corrosion-resistant alloys hardness joinability physical properties Tristelle alloy TS-3 wear resistance thermal...
Journal Articles
Alloy Digest (1996) 45 (11): Co-101.
Published: 01 November 1996
... information on corrosion and wear resistance. Filing Code: CO-101. Producer or source: Stoody Deloro Stellite Inc. Producer or Source: Stoody Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition compressive strength corrosion-resistant alloys...
Journal Articles
Alloy Digest (1994) 43 (12): SS-576.
Published: 01 December 1994
... the aim NOREM 02 chemistry given in Table 1. Table 3 - GALLING WEAR OF GTA WELD OVERLAYS Surface Damage (mm) at Indicated Stress (ksi) Tests in Air Tests in Water Alloy 20 40 60 20 40 60 Deloro 40/nickel-base 37.1 41.3 50.0 17.3 34.7 40.0 Deloro 50/nickel-base 38.6 NT 76.0 14.7 26.4 34.7 Stellire 2l...
Journal Articles
Alloy Digest (1997) 46 (6): Ni-528.
Published: 01 June 1997
... for nuclear plant applications. These alloys have been used in Japanese comnxmial nuclear power plant service for several years. Nucalloy. Stellite@. Debra@, and Stoody@ are registered trademarks of Stoocly Deloro Stellite. Inc. Nucalloy alloys are covered under U.S. Patent No. 4404.049. Chemical Composition...
Journal Articles
Alloy Digest (1993) 42 (6): Co-92.
Published: 01 June 1993
..., hardness, and tensile properties. It also includes information on heat treating, machining, joining, and powder metal forms. Filing Code: CO-92. Producer or source: Deloro Stellite Inc. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical...
Journal Articles
Alloy Digest (1993) 42 (10): Co-94.
Published: 01 October 1993
... be machined, whereas alloys having hardnesses greater Deloro Stellite Inc., St. Louis, MO 63105-(314) 721-5573 In Canada: Deloro Stellite Inc., Belleville. Gntari&613) 968-3481 ...
Journal Articles
Alloy Digest (1993) 42 (8): Co-93.
Published: 01 August 1993
..., hardness, and tensile properties. It also includes information on heat treating, machining, joining, and powder metal forms. Filing Code: CO-93. Producer or source: Deloro Stellite Inc. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical...
Journal Articles
Alloy Digest (1993) 42 (3): Co-90.
Published: 01 March 1993
..., and tensile properties. It also includes information on wear resistance as well as heat treating, machining, joining, and powder metal forms. Filing Code: CO-90. Producer or source: Deloro Stellite Inc. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International...
Journal Articles
Alloy Digest (2019) 68 (12): Co-87.
Published: 01 December 2019
... properties. It also includes information on wear resistance as well as heat treating, machining, and joining. Filing Code: Co-87. Producer or source: Deloro Stellite Inc.. Originally published December 1993, corrected December 2019. Producer or Source: Deloro Stellite Inc. Copyright © ASM International...
Journal Articles
Alloy Digest (1992) 41 (11): Co-86.
Published: 01 November 1992
.... It also includes information on high temperature performance as well as heat treating, machining, and joining. Filing Code: Co-86. Producer or source: Deloro Stellite Inc.. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition...