1-20 of 22 Search Results for

DELORO 15 ALLOYS

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2011) 60 (4): Ni-689.
Published: 01 April 2011
...: Stellite Coatings. Producer or Source: Stellite Coatings Copyright © ASM International® 2011 2011 ASM International chemical composition DELORO 15 ALLOYS DELORO 21 ALLOYS DELORO 22 ALLOYS DELORO 25 ALLOYS hardness molds nickel powder physical properties powder metal products DATA...
Journal Articles
Alloy Digest (2010) 59 (11): Ni-683.
Published: 01 November 2010
... flow rate, sec/50g (sec/0.11 lb) 15 (15) Applications: The alloy was designed for exhaust valves, plungers, seal rings, and other wear applications. Producer: Deloro Stellite Company, Inc. Goshen, Indiana 46526 Tel: (574) 534-2585 Fax: (574) 534-3417 www.stellite.com In UK: Deloro Stellite Swindon SN2...
Journal Articles
Alloy Digest (1969) 18 (5): Ni-145.
Published: 01 May 1969
... Deloro alloy C is a nickel base alloy designed primarily for high corrosion resistance for the chemical industry. It is used for pumps, valves, and hard facing electrodes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1968) 17 (6): Co-55.
Published: 01 June 1968
... DELORO STELLITE-100 is a hard and abrasion resistant alloy designed specifically for metal cutting purposes. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (1993) 42 (3): Ni-424.
Published: 01 March 1993
... DELORO 208 PM is a nickel-base alloy recommended for handling conditions of wear, erosion, heat and corrosion when impact is also a consideration. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1969) 18 (1): Co-57.
Published: 01 January 1969
... DELORO STELLITE 4 is a cobalt-base alloy having high wear resistance, good high temperature strength. It is a machinable casting alloy recommended for hot extrusion and pressing dies, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1993) 42 (7): Ni-435.
Published: 01 July 1993
... DELORO 716 PM is a nickel-base alloy recommended for handling conditions of wear, erosion, heat and corrosion when impact is also a consideration. This datasheet provides information on composition, physical properties, and hardness. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (1994) 43 (12): SS-576.
Published: 01 December 1994
... the aim NOREM 02 chemistry given in Table 1. Table 3 - GALLING WEAR OF GTA WELD OVERLAYS Surface Damage (mm) at Indicated Stress (ksi) Tests in Air Tests in Water Alloy 20 40 60 20 40 60 Deloro 40/nickel-base 37.1 41.3 50.0 17.3 34.7 40.0 Deloro 50/nickel-base 38.6 NT 76.0 14.7 26.4 34.7 Stellire 2l...
Journal Articles
Alloy Digest (1996) 45 (11): Co-101.
Published: 01 November 1996
... information on corrosion and wear resistance. Filing Code: CO-101. Producer or source: Stoody Deloro Stellite Inc. Producer or Source: Stoody Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition compressive strength corrosion-resistant alloys...
Journal Articles
Alloy Digest (2006) 55 (10): Co-114.
Published: 01 October 2006
... phase particles to promote wear resistance while improving corrosion and oxidation resistance over T400. Tribaloy and Stellite are registered trademarks of Deloro Stellite Company, Inc. Weldability: Compared with alloy T-400, T-400C can be weld deposited with plasma transfer arc welding with fewer...
Journal Articles
Alloy Digest (2011) 60 (2): Co-121.
Published: 01 February 2011
... and powder metal forms.Filing Code: Co-121. Producer or source: Stellite Coatings and Deloro Stellite. Producer or Source: Stellite Coatings and Deloro Stellite Copyright © ASM International® 2011 2011 ASM International chemical composition coatings corrosion-resistant alloys hardness...
Journal Articles
Alloy Digest (1993) 42 (6): Co-92.
Published: 01 June 1993
..., hardness, and tensile properties. It also includes information on heat treating, machining, joining, and powder metal forms. Filing Code: CO-92. Producer or source: Deloro Stellite Inc. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical...
Journal Articles
Alloy Digest (1992) 41 (11): Co-86.
Published: 01 November 1992
.... It also includes information on high temperature performance as well as heat treating, machining, and joining. Filing Code: Co-86. Producer or source: Deloro Stellite Inc.. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition...
Journal Articles
Alloy Digest (1993) 42 (10): Co-94.
Published: 01 October 1993
... be machined, whereas alloys having hardnesses greater Deloro Stellite Inc., St. Louis, MO 63105-(314) 721-5573 In Canada: Deloro Stellite Inc., Belleville. Gntari&613) 968-3481 ...
Journal Articles
Alloy Digest (1993) 42 (8): Co-93.
Published: 01 August 1993
..., hardness, and tensile properties. It also includes information on heat treating, machining, joining, and powder metal forms. Filing Code: CO-93. Producer or source: Deloro Stellite Inc. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical...
Journal Articles
Alloy Digest (2019) 68 (12): Co-87.
Published: 01 December 2019
... properties. It also includes information on wear resistance as well as heat treating, machining, and joining. Filing Code: Co-87. Producer or source: Deloro Stellite Inc.. Originally published December 1993, corrected December 2019. Producer or Source: Deloro Stellite Inc. Copyright © ASM International...
Journal Articles
Alloy Digest (1993) 42 (3): Co-90.
Published: 01 March 1993
..., and tensile properties. It also includes information on wear resistance as well as heat treating, machining, joining, and powder metal forms. Filing Code: CO-90. Producer or source: Deloro Stellite Inc. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International...
Journal Articles
Alloy Digest (1993) 42 (4): Co-91.
Published: 01 April 1993
..., and tensile properties. It also includes information on wear resistance as well as heat treating, machining, joining, and powder metal forms. Filing Code: CO-91. Producer or source: Deloro Stellite Inc. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International...
Journal Articles
Alloy Digest (1982) 31 (3): Ni-274.
Published: 01 March 1982
... STELLlTE* alloy No. 6 has been used successfully. *HAYNES, STELLITE and DELORO are @&red trademarks of Cabot Corporation. [The properties listed herein are based on laboratory tests by the manufachuer and should not be used for specification or final design. The secondary units (metric) are those of the SI...
Journal Articles
Alloy Digest (1967) 16 (3): Co-51.
Published: 01 March 1967
... % Nehring, Krefeld, Germany Jadot Freres, Beloeill, Belguim Fonderies Magotteaux, Liege, Belguim Fagersta Bruks A.B., Fagersta, Sweden Samuel Osborne % Co. Ltd., Sheffield, England Societe Metallurgique d Imphy, Paris, France Acierie & Fonderie de Haute Sambre, Berlaimont, France Deloro Stellite Ltd...