Journal Articles
Alloy Digest (2003) 52 (1): TS-599.
Published: 01 January 2003
... DC53 can be hardened up to 63 HRC without losing toughness or becoming brittle. It is a long-lasting steel that reduces cracking and chipping and often replaces D2. This datasheet provides information on composition, physical properties, hardness, elasticity, and shear strength as well as fracture...