Alloy Digest (1991) 40 (7): Cu-562.
Published: 01 July 1991
... CBX CUPRON ALLOY is a resistance alloy with practically constant resistance over the range of -67 to 221 F. The alloy does not generate gas when in contact with glass, enamel or ceramic type materials, an advantage over CB CUPRON (Constantan). This datasheet provides information on composition...
Journal Articles
Alloy Digest (1992) 41 (1): Cu-568.
Published: 01 January 1992
... CUPRON Alloy is the standard negative thermoelement used with copper, with iron and with TOPHEL Alloy in ISA Types T, J and E thermocouples, respectively. PCLW-SNX and PCLW-BPX are thermocouple extension wire alloys. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1962) 11 (10): Cu-121.
Published: 01 October 1962
... Cupron is a copper-nickel resistance alloy recommended for maximum operating temperature of 1000 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. Filing Code: Cu-121. Producer or source: Wilbur B. Driver Company. Producer...
Journal Articles
Alloy Digest (2015) 64 (10): Cu-842.
Published: 01 October 2015
... 100 °C (77 212 °F), °C 1 (°F 1) Thermal coefficient of expansion, 25 100 °C (77 212 °F), 10 6/K (10 6/°F) Thermal conductivity, W/m·K (Btu/(h·ft·ºF)) Cupron 1210 (2210) 393 (0.094) 8900 (0.320) 0.5 (300) ± 40 (± 22) 14.9 (8.3) 21.3 (11.8) Tophel 1427 (2600) 460 (0.110) 8630 (0.317) 0.7 (410) 390 (217...
Journal Articles
Alloy Digest (2019) 68 (5): Ni-751.
Published: 01 May 2019
... / 3.25 mm (0.128 in.) 14 / 1.63 mm (0.064 in.) 20 / 0.81 mm (0.032 in.) 24 / 0.51 mm (0.020 in.) 28 / 0.33 mm (0.013 in.) °C (°F) °C (°F) °C (°F) °C (°F) °C (°F) Tophel-Cupron E 871 (1600) 649 (1200) 537 (999) 427 (801) 427 (800) Tophel-NIAL K 1269 (2316) 1093 (2000) 982 (1800) 871 (1600) 871 (1600...
Journal Articles
Alloy Digest (2012) 61 (2): Cu-803.
Published: 01 February 2012
...) Specific heat, 20 ºC (68 ºF), J/kg·K (Btu/lb·ºF) Density, kg/m3 (lb/in.3) Resistivity, 25 ºC (77 ºF), m ( circular-mil/ft) CUPRON 1210 (2210) 393 (0.094) 8900 (0.320) 0.50 (300) TOPHEL 1427 (2600) 480 (0.11) 8630 (0.311) 0.68 (410) NIAL 1399 (2550) 502 (0.12) 8470 (0.305) 0.32 (193) NICROSIL 1410 (2570...
Journal Articles
Alloy Digest (1992) 41 (1): Ni-400.
Published: 01 January 1992
... OF THERMOCOUPLES ISA MOY Temperature Range Limit of Error Type Pair C OF Standard Special K TOPHEL@/NIAL 0- 1250 (32-2282) ti.2pc f 1.3/q f 1.1 C (H.6 F) or +.75% or ti.4* E TOPHEL@/CUPRON@ O-900 (32-1652) f1.7 C (H°F) +0.83 C (H.6 l=) or !zO.50% or 0.4%* *% of the actuai temperature, not temperature range...
Journal Articles
Alloy Digest (1995) 44 (7): Cu-602.
Published: 01 July 1995
... by the purchaser, this should be stated at the inquiry/order stage. The thermal. electrical, mechanical properties, and modulus of elasticity of MARINEL are similar to those of 70/30 cupron- ickel. MARINEL is of slightly lower density, however (5% less), and also has 2 to 3 times the hardness of conventional...
Journal Articles
Alloy Digest (1995) 44 (6): Cu-601.
Published: 01 June 1995
..., flanges and ether critical high strength components and finds wide application in surface and subsea vessels and on offshore oil and gas platforms. lhe alloy has the inherent good resistance to bio-fouling of a cupron- ickel while the additional elements in its compositiar not only improve mechanical...