1-1 of 1 Search Results for

Cunisil-837

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1961) 10 (7): Cu-104.
Published: 01 July 1961
... Cunisil-837 is a copper-nickel-silicon alloy having high strength and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing...