Alloy Digest (2019) 68 (7): TS-771.
Published: 01 July 2019
... Cryodur 2842 is a cold work tool steel for cutting, punching, and folding. This datasheet provides information on composition and physical properties. It also includes information on heat treating and joining. Filing Code: TS-771. Producer or source: Schmolz + Bickenbach USA Inc.. Producer...