Alloy Digest (2013) 62 (2): SA-670.
Published: 01 February 2013
... Cryelso 3.5 is a steel alloy designed for low temperature applications and requiring high impact values. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on low temperature performance as well as forming, heat...