Alloy Digest (2011) 60 (10): SS-1104.
Published: 01 October 2011
...-resistant alloys Crucible CPM S110V heat treatability machinability microstructure wear resistance DATA ON WORLDWIDE METALS AND ALLOYS Copyright ┬ę 2011, ASM International┬«. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM International...
Journal Articles
Alloy Digest (2022) 71 (8): TS-830.
Published: 01 August 2022
... Crucible CPM S110V is a high alloy martensitic stainless tool steel produced by the Crucible Particle Metallurgy (CPM) process. Crucible CPM S110V contains a high volume fraction of both vanadium-rich and niobium-rich primary alloy carbides for exceptionally good wear resistance compared to other...