Alloy Digest (2009) 58 (2): SA-593.
Published: 01 February 2009
... CromElso 11 is a specially designed low-alloy steel for high-temperature hydrogen service, particularly hydrotreating reactors. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on high temperature performance...