Alloy Digest (1967) 16 (11): SS-202.
Published: 01 November 1967
... Croloy 16-13-3 is a molybdenum-containing 18-12 type austenitic stainless steel having better corrosion resistance than the 18-8 type stainless steels. It is recommended for corrosion resisting applications in the chemical and oil refinery industries, paper pulp processing, etc. In addition...
Journal Articles
Alloy Digest (1966) 15 (4): SS-180.
Published: 01 April 1966
... 120-135 35-62 102-110 38-44 Norm. % Tempered As welded As welded Norm. & Temp. t 135OoF SR 135OOF SR 13500F SR Welded t SR 1300oF Welded t SR 13000F Welded + SR 14250F Welded + SR 11500F Welded t SR 12000F 41-47 100-107 35-55 50-55 2-3 8-33-45 o-4 3-4 7-13 16-19 17-20 +40oF t 1OoF -2OoF -500F - - 85...