Alloy Digest (1965) 14 (6): Cu-152.
Published: 01 June 1965
... Cramp Superstrength No. 49 is a special bronze alloy with high mechanical properties. It is recommended for castings and forgings subject to high compressive loads and shock. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...