Skip Nav Destination
Close Modal
Search Results for
Copper alloy no. C87400
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
Copper alloy no. C87400
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1986) 35 (2): Cu-506.
Published: 01 February 1986
... Copper Alloy No. C87400 is a copper-base casting alloy containing nominally 14% zinc and 3.5% silicon. It possesses a combination of high strength, good ductility and good-to-excellent resistance to corrosion. This alloy cannot be hardened nor strengthened by any thermal treatment. It is used...
Abstract
View article
PDF
Copper Alloy No. C87400 is a copper-base casting alloy containing nominally 14% zinc and 3.5% silicon. It possesses a combination of high strength, good ductility and good-to-excellent resistance to corrosion. This alloy cannot be hardened nor strengthened by any thermal treatment. It is used for numerous applications such as bearings, gears, impellers and valve stems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-506. Producer or source: Copper alloy foundries.