Alloy Digest (1987) 36 (8): Cu-527.
Published: 01 August 1987
... Copper Alloy No. C82600 is an age-hardenable copper-base casting alloy. Nominally it contains 2.3% beryllium. It is characterized by high strength, toughness and good corrosion resistance. Typical uses comprise bearings and molds for plastics. This datasheet provides information on composition...