Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (6): Cu-553.
Published: 01 June 1990
... Copper alloy No. C76390 is a wrought (rod) leaded nickel silver with nominally 24.5% nickel and 1% lead. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-553...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (11): Cu-914.
Published: 01 November 2020
..., but not less than 1 h. Air or furnace cool. Heat treat- ment information sourced from L. Klein SA, Lebronze Alloys, and Copper Development Association. Chemical Composition Element Composition, wt%(a) L. Klein ARCAP AP1D UNS C76390(b) UNS C79350(c) Copper 59.0 63.0 59.0 63.0(d) 59.0 63.0(d)(e) Nickel 23.0 26.0...