Alloy Digest (1991) 40 (2): Cu-557.
Published: 01 February 1991
... Copper Alloy No. C70600 is a very resistant alloy in a seawater service. Failure in properly designed systems in such environments by general corrosion, pitting, crevice attack and stress-cracking can be discounted for this copper nickel alloy. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1982) 31 (12): Cu-449.
Published: 01 December 1982
... also increases. Iron additions IO the composi- tion further improve erosion-corrosion resistance. as is the case with Copper Alloy No. C70600 (90-10 copper-nickel). Additional improvement is provided by Copper Alloy No. C72200. with its in- termediate nickel level (15%) in combination with both iron...
Journal Articles
Alloy Digest (2019) 68 (7): Cu-892.
Published: 01 July 2019
.... Product Forms Availableb Sheet, strip, ingot, rod, and tube. Applications CuVerro antimicrobial copper begins killing infectious bacteria on contact and keeps killing it, and unlike stainless steel and silver-based coating, the material continuously destroys and eliminates bacteria between cleaning no...
Journal Articles
Alloy Digest (1985) 34 (10): Cu-501.
Published: 01 October 1985
.... C70600. ASME: SB I II, SB 466 and SB 467. ASTM: B I 11, B 466, B 467 and B 552. SAE: 5461 and 3463. UNS No. C70600. Military: MIL-T-15005 and MIL-T-16420. General Characteristics: Mueller Alloy 7060 (nominally IO% nickel) was developed to meet the requirements for a lower cost metal than 70130 copper...
Journal Articles
Alloy Digest (1980) 29 (3): Cu-391.
Published: 01 March 1980
... containing air bubbles and silt flowing at high velocities. Specification Equivalents: ASTM: B 111, B 171, B 395 and B 402. SAE CA 706. Military: MILC-15726, MIL-T-16420 and MIL-T-15005. CDA Copper Alloy No. 706. UNS No. C70600. General Characteristics: Anaconda alloy 706 is the low-nickel member of the...