Alloy Digest (1990) 39 (2): Cu-550.
Published: 01 February 1990
... International chemical composition Copper alloy no. C61900 elasticity fatigue properties hardness heat treatability joinability machinability physical properties tensile properties workability UNS C61900 COPPER ALLOY No. 61900 e%ty cu-55o -DIGEST FEBRUARY 1990 - DATA ON WORLD WIDE METALS...