Skip Nav Destination
Close Modal
Search Results for
Copper alloy no. C42200
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-4 of 4 Search Results for
Copper alloy no. C42200
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1984) 33 (8): Cu-482.
Published: 01 August 1984
... Copper Alloy No. C42200 is brass with an addition of tin (nominally 1.1%). It can be machined, formed and joined successfully. It has good resistance to corrosion. Typical uses include terminals, fuse clips, contact springs and electrical connectors. This datasheet provides information...
Abstract
View article
PDF
Copper Alloy No. C42200 is brass with an addition of tin (nominally 1.1%). It can be machined, formed and joined successfully. It has good resistance to corrosion. Typical uses include terminals, fuse clips, contact springs and electrical connectors. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on heat treating. Filing Code: Cu-482. Producer or source: Copper and copper alloy mills.
Journal Articles
Alloy Digest (2020) 69 (1): Cu-904.
Published: 01 January 2020
... Olin Brass Alloy C42200 (Tradename: Lubronze) is a copper-zinc-tin alloy (tin brass). The mechanical properties and performance of C42200 are very similar to those of high-zinc brass alloys with the added benefit of improved resistance to stress relaxation. It is also a cost-effective alternative...
Abstract
View article
PDF
Olin Brass Alloy C42200 (Tradename: Lubronze) is a copper-zinc-tin alloy (tin brass). The mechanical properties and performance of C42200 are very similar to those of high-zinc brass alloys with the added benefit of improved resistance to stress relaxation. It is also a cost-effective alternative to phosphor bronze. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well as forming. Filing Code: Cu-904. Producer or source: Olin Brass GBC Metals, LLC.
Journal Articles
Alloy Digest (2009) 58 (2): Cu-765.
Published: 01 February 2009
... elasticity electrical conductivity electrical contacts hardness heat treatability joinability LUVATA C422 machinability physical properties tensile properties thermal conductivity workability UNS C42200 LUVATA C422 (Copper Alloy) Luvata C422 is a copper alloy with good spring properties...
Abstract
View article
PDF
Luvata C422 is a copper alloy with good spring properties and good electrical and thermal conductivity used in electrical contacts. It is often called Ambronze 422. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on forming, heat treating, machining, and joining. Filing Code: CU-765. Producer or source: Luvata Sales (USA) Inc.
Journal Articles
Alloy Digest (1999) 48 (9): Cu-639.
Published: 01 September 1999
... springs tensile properties workability WRM alloy 4222 thermal properties UNS C42200 WRM ALLOY 4222 (Tin Brass Alloy) WRM alloy 4222 is a copper-zinc-tin alloy of the tin-brass family with a good combination of conductivity, strength, and forming characteris- tics. A typical application is in high...
Abstract
View article
PDF
WRM alloy 4222 is a copper-zinc alloy of the tin-brass family with a good combination of conductivity, strength, and forming characteristics. A typical application is in high-performance conductive springs. This datasheet provides information on composition, physical properties, tensile properties. and bend strength. It also includes information on forming. Filing Code: CU-639. Producer or source: Waterbury Rolling Mills Inc.