Alloy Digest (1982) 31 (3): Cu-433.
Published: 01 March 1982
... Copper Alloy No. C35300 is a high-leaded brass (nominally 1.8% lead) that is noted for its excellent thread-rolling and knurling properties. It has a machinability rating approaching that of Free-Cutting Brass (Copper Alloy No. C36000). It is used in many screw-machine applications and has good...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (7): Cu-398.
Published: 01 July 1980
... No. C35300. CDA Copper Alloy No. C35300. General Characteristics: Mueller alloy 3530 is a wrought copper alloy containing nominally 61% copper, 1.7% lead and the remainder zinc. This ahoy cannot be hardened or strengthened by any thermal treatment but it can be hardened by cold working. After cold working...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (3): Cu-796.
Published: 01 March 2011
..., machining, and joining. Filing Code: Cu-796. Producer or source: Ansonia Copper & Brass. Producer or Source: Ansonia Copper & Brass Copyright © ASM International® 2011 2011 ASM International ANSONIA ALLOY C35300 chemical composition elasticity hardness heat treatability joinability...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (1): Cu-657.
Published: 01 January 2001
... elasticity hardness heat treatability joinability machinability physical properties Swissmetal SM184N (Boillat 62A) tensile properties workability thermal properties UNS C34500 C35300 Swissmetal SM184N is a free-machining brass alloy with an optimal combination of machinability and cold...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (6): Cu-683.
Published: 01 June 2002
... International chemical composition corrosion-resistant alloys elasticity hardness heat treatability joinability machinability physical properties Swissmetal alloy SM158N (Boillat 61B) tensile properties workability thermal properties UNS C35300 Composition, wt Copper 61.10 62.00 Lead 1.6...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (5): Cu-908.
Published: 01 May 2020
... Mueller Brass Alloy C34500 is a copper-zinc-lead (leaded brass) alloy that is suitable for applications requiring extensive machining before cold-forming operations such as swaging, flaring, severe knurling, or thread rolling. This datasheet provides information on composition, physical properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (12): Cu-908a.
Published: 01 December 2020
... Mueller Brass Alloy C34500 is a copper-zinc-lead (leaded brass) alloy that is suitable for applications requiring extensive machining before cold-forming operations such as swaging, flaring, severe knurling, or thread rolling. Melting temperature values corrected December 2020. This datasheet...