Alloy Digest (1984) 33 (5): Cu-476.
Published: 01 May 1984
... Copper Alloy No. C34200 contains nominally 2% lead and has a machinability rating approaching that of Free-Cutting Brass. It is noted for its excellent thread-rolling and knurling properties. It is used for many screw-machine applications and it has good resistance to corrosion in many...