Journal Articles
Alloy Digest (1981) 30 (4): Cu-415.
Published: 01 April 1981
... Copper Alloy No. C34000 is a medium-leaded brass characterized by an excellent combination of free-machining and cold-working properties. It is intended for screw-machine applications where excellent thread-rolling, knurling, machining and cold-forming properties are required. Among its many...
Journal Articles
Alloy Digest (1979) 28 (9): Cu-379.
Published: 01 September 1979
...- pounds, moist ammonia, cyanides and strong bases should be avoided. Specification Equivalents: ASTM B 453 (Copper Alloy 340). UNS No. C34000. CDA No. 340. General Characteristics: Mueller alloy 3406 is a medium-leaded brass containing nominally 64.5% copper, I % lead and remainder zinc. It combines...