Alloy Digest (1985) 34 (4): Cu-496.
Published: 01 April 1985
... Copper Alloy No. C33500 is a brass containing 0.5% lead. It is used where moderate cold working and/or some machining is required. It possesses fair capacity for welding. It is used in a wide variety of hardware items. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2002) 51 (11): Cu-693.
Published: 01 November 2002
... International chemical composition corrosion-resistant alloys elasticity hardness heat treatability joinability physical properties Swissmetal alloys SM185N Swissmetal alloys SM188N tensile properties workability thermal properties UNS C34400 C33500 Composition, wt SM185N SM188N Copper 62.8...