Alloy Digest (1990) 39 (12): Cu-556.
Published: 01 December 1990
... Copper alloy C32000 is a leaded red brass applicable to automatic screw machine production of parts for hardware and industrial applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue...