Journal Articles
Alloy Digest (1980) 29 (1): Cu-387.
Published: 01 January 1980
... Copper Alloy No. 932 is a cast bronze containing nominally 7% lead and 7% tin. Commercial names formerly used (not recommended) are (1) High-Leaded Tin Bronze, (2) Bearing Bronze 660 and 83-7-7-3. It has relatively low strength, good machinability and good resistance to corrosion. Its uses include...
Journal Articles
Alloy Digest (2022) 71 (7): Cu-932.
Published: 01 July 2022
...-2.5Ni-0.65Si-0.35Cr Alloy) Filing Code: Cu-932 Copper :: July 2022 Materials Park, Ohio 44073-0002, USA :: +1.440.338.5151 :: www.asminternational.org :: matinfo@asminternational.org Published by ASM International® :: Data shown are typical, not to be used for specification or final design...
Journal Articles
Alloy Digest (1977) 26 (4): Cu-330.
Published: 01 April 1977
... physical properties tensile properties All 08 BUNTING Alloy 932 Filing Code: a-330 Copper Alloy APRIL 1977 DICESid - DATA ON WORLD WIDE METALS AND ALLOYS p#&b8d by BUNTING* Alloy 932 (High-Leaded Tin Bronze) BUNTING Alloy 932 is a cast bearing and bushing bronze. It has excellent anti-friction...
Journal Articles
Alloy Digest (1992) 41 (5): Cu-571.
Published: 01 May 1992
... material. Composltlon (Nominal): Copper Tin Lead Zinc 83 7 7 3 Physical Properties:* Density, Ib/cu in. Mg/cu m Liquidus , F C Solidus, F C Incipient melting temperature (Pb), OF C Thermal coef. of expansion, (32 to 212 FF (0 to 100°C) Thermal conductivity @ 68OF, Btu/ft=he F @ 20°C W/m-K Electrical...
Journal Articles
Alloy Digest (1997) 46 (5): Cu-613.
Published: 01 May 1997
...: Copper Alloy No. C89835 General Characteristics: The basis for developing lead-free Federalloy is twofold. Re- moving lead eliminates the health issues associated with leaching lead from plumbing fixtures into water and meets the new OSHA standard for airborne lead (50 pg/m3) in nonfer- rous foundries...
Journal Articles
Alloy Digest (2010) 59 (10): Cu-791.
Published: 01 October 2010
... at temperatures of more than 500 ºC (932 ºF) Konstantan is liable to intergranular corrosion. Specification Equivalents: DIN 17644, 17670, 17471, 17672, 17677, 46339, 46460, 46461, 46462, 46464 ASTM B267 General Characteristics: Konstantan is a copper-nickel alloy with 44% nickel and 0.5 to 2% manganese...
Journal Articles
Alloy Digest (2013) 62 (12): Cu-828.
Published: 01 December 2013
... Ansonia alloy ACB C18150 is an age-hardenable zirconium chromium copper alloy with high electrical conductivity, hardness, and ductility; moderate strength; and excellent resistance to softening at elevated temperatures. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2015) 64 (2): Ni-720.
Published: 01 February 2015
... 696 tensile properties workability UNS N06696 NSSMC 696 is a high-temperature alloy with noted resistance to metal dusting. Chemical Composition, wt (Maximum) Chromium 28.00 32.00 Phosphorus 0.040 Sulfur 0.010 Nitrogen 0.025 Copper 1.5 3.0 Molybdenum 1.0 3.0 Manganese 1.0 Silicon 1.0 2.5 Carbon...
Journal Articles
Alloy Digest (1970) 19 (12): Cu-224.
Published: 01 December 1970
... International chemical composition Coronze alloy 638 corrosion-resistant alloys elasticity fatigue properties heat treatability high-temperature alloys joinability machinability physical properties tensile properties workability CORONZE Alloy 638 Filing Code: Cu-224 Copper Alloy DECEMBER 1970...
Journal Articles
Alloy Digest (1999) 48 (7): SS-747.
Published: 01 July 1999
... of Special Metal Corp. Chemical Composition, wt (Typical) Carbon 0.020 Chromium 20 Nickel 25 Molybdenum 4.3 Nitrogen 0.13 Copper 1.5 Iron Balance Using the PREN equation, the alloy is designed to have a PREN 36. Physical Properties: Density, kg/m3 (lb/in.3) 8050 (0.29) Coefficient of thermal expansion, 10 6...
Journal Articles
Alloy Digest (2014) 63 (1): Cu-830.
Published: 01 January 2014
... Ansonia alloy ACB C18900 was developed to be able to make the finest welds possible in copper. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: Cu-830. Producer...
Journal Articles
Alloy Digest (2008) 57 (10): SS-1019.
Published: 01 October 2008
... power stations using steam temperatures of up to approximately 600 °C (1112 °F) in supercritical and ultrasupercritical vessel designs. Austenitic stainless steel alloyed with copper and boron to increase the creep strength, has very good high-temperature corrosion resistance, and very good creep...
Journal Articles
Alloy Digest (2023) 72 (6): Ni-783.
Published: 01 June 2023
... has high strength, good metallurgical stability, and favorable fabrication characteristics. Chemical Composition Element Nickel Chromium Cobalt Iron Manganese Carbon Copper Silicon Sulfur Composition, wt%(a) Aubert & Duval NY690 Alloy N06690 bal 58.0 30.0 27.0 31.0 (b) 10.0 7.0 11.0 0.5 0.05...
Journal Articles
Alloy Digest (2015) 64 (4): SS-1205.
Published: 01 April 2015
... and discs, shafts, pins, bolts, screws, springs, exhaust reheaters, housing components, thrust nozzles. Liners for containers for tube and rod extruding of copper and copper-alloys; billet temperature higher than 700 °C (1292 °F). Producer: Böhler-Uddeholm Specialty Metals, Inc. South Boston, VA 24592, USA...
Journal Articles
Alloy Digest (1990) 39 (3): Cu-551.
Published: 01 March 1990
... Zirconium Copper is an age hardenable electrical conductivity alloy which develops high strength when heat treated. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (1998) 47 (1): Al-345.
Published: 01 January 1998
... Aluminium-Copper Matrix Composites aluminum-matrix composites chemical composition compressive strength corrosion-resistant alloys elasticity fatigue properties physical properties shear strength tensile properties thermal properties - DIGEST d 3M ALUMINUM-2 wt.% Cu Matrix ComDosites DATA...
Journal Articles
Alloy Digest (2016) 65 (12): SA-774.
Published: 01 December 2016
... 0.75 Phosphorus 0.020 max Sulfur 0.020 max Aluminum, total 0.015 0.080 Boron 0.001 0.010 Chromium 0.90 1.20 Molybdenum 0.90 1.10 Nickel 0.20 max Vanadium 0.60 0.80 Titanium 0.07 0.15 Arsenic 0.020 max Tin 0.020 max Copper 0.20 max Antimony report R* 0.1 max *R = P + 2.43As + 3.57Sn + 8.16Sb + 0.13Cu...
Journal Articles
Alloy Digest (2001) 50 (6): Cu-668.
Published: 01 June 2001
... Swissmetal SM453C is a free-machining copper alloy with high electrical conductivity. It is recommended for male contacts in electrical and electronic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2014) 63 (5): SS-1174.
Published: 01 May 2014
... max Nitrogen 0.15 0.35 Niobium 0.20 0.60 Manganese 2.00 max Copper 1.00 max Carbon 0.04 0.10 Iron bal Physical Properties: Density, kg/cm3 (lb/in.3) 8100 (0.29) Coefficient of thermal expansion, 10 6/K (10 6/°F) RT 300 °C (RT 572 °F) 16.9 (9.4) RT 400 °C (RT 752 °F) 17.2 (9.6) RT 500 °C (RT 932 °F...
Journal Articles
Alloy Digest (2018) 67 (9): SS-1293.
Published: 01 September 2018
... 23.5 Nickel 23.5 26.5 Tungsten 2.0 4.0 Cobalt 1.0 2.0 Copper 2.0 3.5 Niobium 0.30 0.60 Boron 0.002 0.008 Nitrogen 0.15 0.30 Iron bal Physical Properties Density, kg/m3 (lb/in.3) 8100 (0.29) Thermal conductivity, W/m·K (Btu/(h·ft·°F)) 20 °C (68 °F) 12 (6.9) 500 °C (932 °F) 20 (11.6) 800 °C (1472 °F) 25...