Skip Nav Destination
Close Modal
Search Results for
Copper alloy no. 923
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-13 of 13
Search Results for Copper alloy no. 923
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1978) 27 (6): Cu-355.
Published: 01 June 1978
... Copper Alloy No. 923 is a cast copper-tin-zinc-lead alloy known also as Leaded G Bronze or 87-8-1-4 alloy. This alloy possesses a good combination of strength, resistance to corrosion and machinability. It is a good alloy to withstand gas or liquid pressures. Applications include pump impellers...
Abstract
View articletitled, <span class="search-highlight">COPPER</span> <span class="search-highlight">ALLOY</span> No. <span class="search-highlight">923</span>: Cast Leaded Tin Bronze
View
PDF
for article titled, <span class="search-highlight">COPPER</span> <span class="search-highlight">ALLOY</span> No. <span class="search-highlight">923</span>: Cast Leaded Tin Bronze
Copper Alloy No. 923 is a cast copper-tin-zinc-lead alloy known also as Leaded G Bronze or 87-8-1-4 alloy. This alloy possesses a good combination of strength, resistance to corrosion and machinability. It is a good alloy to withstand gas or liquid pressures. Applications include pump impellers, fittings and bearings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-355. Producer or source: Copper alloy foundries.
Journal Articles
Alloy Digest (1979) 28 (2): Cu-367.
Published: 01 February 1979
... BUNTING Alloy 923 is a cast copper-tin-lead-zinc alloy that possesses a good combination of machinability, strength and resistance to corrosion. It is known also as 87-8-1-4 alloy or Leaded G Bronze. It withstands gas or liquid pressures quite successfully. Its numerous applications include valves...
Abstract
View articletitled, BUNTING <span class="search-highlight">ALLOY</span> <span class="search-highlight">923</span>: Cast Leaded Tin Bronze
View
PDF
for article titled, BUNTING <span class="search-highlight">ALLOY</span> <span class="search-highlight">923</span>: Cast Leaded Tin Bronze
BUNTING Alloy 923 is a cast copper-tin-lead-zinc alloy that possesses a good combination of machinability, strength and resistance to corrosion. It is known also as 87-8-1-4 alloy or Leaded G Bronze. It withstands gas or liquid pressures quite successfully. Its numerous applications include valves, gears and bushings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-367. Producer or source: NL Industries Inc., Bearing Division.
Journal Articles
Alloy Digest (2021) 70 (8): Cu-923.
Published: 01 August 2021
... properties tensile properties thermal properties workability UNS C12200 KME Cu-DHP (Phosphorus-Deoxidized Copper, High Residual Phosphorus) Filing Code: Cu-923 Copper :: August 2021 Materials Park, Ohio 44073-0002, USA :: +1.440.338.5151 :: www.asminternational.org :: [email protected]...
Abstract
View articletitled, KME Cu-DHP: Phosphorus-Deoxidized <span class="search-highlight">Copper</span>, High Residual Phosphorus
View
PDF
for article titled, KME Cu-DHP: Phosphorus-Deoxidized <span class="search-highlight">Copper</span>, High Residual Phosphorus
KME Cu-DHP is a phosphorus-deoxidized copper that contains a minimum of 99.90% copper and high residual phosphorus. The electrical conductivity of this type of copper is relatively low on account of the high phosphorus content. KME Cu-DHP possesses very good formability and joining properties and is resistant against hydrogen embrittlement. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-923. Producer or source: KME Germany GmbH.
Journal Articles
Alloy Digest (2008) 57 (9): Al-417.
Published: 01 September 2008
... joinability machinability physical properties tensile properties workability ALCAN 2024-T3, T351X (Aluminum-Copper-Magnesium Alloy Extruded Bar) This datasheet covers Alcan 2024 alloy in T3 and T351x tempers. The alloy possesses good damage tolerance. Chemical Composition, wt (Typical) Silicon 0.50 max...
Abstract
View articletitled, ALCAN 2024-T3, T351X: Aluminum-<span class="search-highlight">Copper</span>-Magnesium <span class="search-highlight">Alloy</span> Extruded Bar
View
PDF
for article titled, ALCAN 2024-T3, T351X: Aluminum-<span class="search-highlight">Copper</span>-Magnesium <span class="search-highlight">Alloy</span> Extruded Bar
This datasheet covers Alcan 2024 alloy in T3 and T351x tempers. The alloy possesses good damage tolerance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: AL-417. Producer or source: Alcan Inc.
Journal Articles
Alloy Digest (1999) 48 (7): Ni-555.
Published: 01 July 1999
... Molybdenum 8.0 10.0 Iron 5.0 max Carbon 0.10 max Aluminum 0.40 max Titanium 0.40max Cobalt 0.10 max Copper 0.50 max Manganese 0.50 max Phosphorus 0.015 max Silicon 0.50 max Sulfur 0.015 max Nickel Balance Properties: P/M N625 exhibits isotropic mechanical properties and excellent corrosion resistance. Table...
Abstract
View articletitled, CRUCIBLE P/M N625: Powder Metallurgy (P/M) Corrosion-Resistant Nickel-<span class="search-highlight">Alloy</span>
View
PDF
for article titled, CRUCIBLE P/M N625: Powder Metallurgy (P/M) Corrosion-Resistant Nickel-<span class="search-highlight">Alloy</span>
Crucible P/M N625 is a powder metallurgical nickel-base alloy with excellent corrosion resistance, high strength, chemical homogeneity, and thermal stability. Applications include use for highly corrosive situations in the marine, nuclear power, pulp and paper, and chemical process industries. This datasheet provides information on composition, microstructuretensile properties. It also includes information on powder metal forms. Filing Code: Ni-555. Producer or source: Crucible Compaction Metals.
Journal Articles
Alloy Digest (2010) 59 (6): Al-429.
Published: 01 June 2010
... This datasheet covers Alcan 2024 alloy in T3 and T351x tempers for drawn tubes. The alloy possesses good damage tolerance. See also Alloy Digest Al-417. ALCAN 2024 T3, T351X TUBES (Aluminum-Copper- Magnesium Alloy) ALCAN 2024 T3, T351X TUBES Chemical Composition, wt (Typical) Silicon 0.50 max Iron 0.50 max...
Abstract
View articletitled, ALCAN 2024 T3, T351X TUBES: Aluminum-<span class="search-highlight">Copper</span>- Magnesium <span class="search-highlight">Alloy</span>
View
PDF
for article titled, ALCAN 2024 T3, T351X TUBES: Aluminum-<span class="search-highlight">Copper</span>- Magnesium <span class="search-highlight">Alloy</span>
This datasheet covers Alcan 2024 alloy in T3 and T351x tempers for drawn tubes. The alloy possesses good damage tolerance. See also Alloy Digest Al-417, September 2008, for information about this alloy in extruded bar form. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: AL-429. Producer or source: Alcan Inc., Alcan Aerospace.
Journal Articles
Alloy Digest (2005) 54 (6): SS-923.
Published: 01 June 2005
... physical properties tensile properties thermal properties UNS N08367 Composition, wt (Typical) AL-6XN AL-6XN PLUS Carbon 0.02 0.02 Manganese 0.40 0.30 Phosphorus 0.020 0.020 Sulfur <0.001 <0.001 Silicon 0.40 0.35 Chromium 20.5 21.8 Nickel 24.0 25.3 Molybdenum 6.2 6.7 Nitrogen 0.22 0.24 Copper 0.2 0.2...
Abstract
View articletitled, ALLEGHENY LUDLUM AL-6XN PLUS: Superaustenitic Stainless Steel
View
PDF
for article titled, ALLEGHENY LUDLUM AL-6XN PLUS: Superaustenitic Stainless Steel
The AL-6XN PLUS alloy is an enhanced version of the AL-6XN alloy (see Alloy Digest SS-494, May 1988). Both satisfy the composition requirements of UNS N08367, but AL-6XN PLUS contains a greater concentration of the alloying elements (Cr, Mo, and N) which promote corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as heat treating and joining. Filing Code: SS-923. Producer or source: Allegheny Ludlum Corporation. Originally published April 2005, revised June 2005.
Journal Articles
Alloy Digest (1993) 42 (8): Ni-439.
Published: 01 August 1993
... content provides superior resistance to IGSCC. This alloy has superb weldability characteristics as well as minimal mechanical property degradation during extended exposure to elevated temperatures. Composition, Wt, %: Chromium Iron Carbon Silicon Manganese Sulfur Copper Nickel 28.0-3 1 .O 7.0-l 1.0 0.04...
Abstract
View articletitled, CRUCIBLE P/M N690: Corrosion Resistant High Chromium Nickel <span class="search-highlight">Alloy</span>
View
PDF
for article titled, CRUCIBLE P/M N690: Corrosion Resistant High Chromium Nickel <span class="search-highlight">Alloy</span>
P/M N690 exhibits isotropic mechanical properties and excellent corrosion resistance. Its high chromium content provides superior resistance to IGSCC. This alloy has superb weldability characteristics as well as minimal mechanical property degradation during extended exposure to elevated temperatures. This datasheet provides information on composition, microstructuretensile properties. It also includes information on corrosion resistance. Filing Code: Ni-439. Producer or source: Crucible Compaction Metals.
Journal Articles
Alloy Digest (2018) 67 (12): SS-1300.
Published: 01 December 2018
... Sulfur 0.005 Chromium 15.0 17.0 Nickel 4.0 5.0 Molybdenum 0.8 1.2 Copper 0.5 Nitrogen 0.020 Iron bal Physical Properties Density, kg/m3 (lb/in.3) Condition A/H11 7750 (0.279) Condition H1150 7860 (0.283) Weight of round bars, kg/m (lb/in.) Condition A/H1150 0.0062 (0.000347) × diam2 Weight of round bars...
Abstract
View articletitled, UGI 4542 AIR: Martensitic Stainless Steel
View
PDF
for article titled, UGI 4542 AIR: Martensitic Stainless Steel
UGI 4542 AIR is a martensitic precipitation hardening stainless steel with strong corrosion resistance and high mechanical performance. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1300. Producer or source: Schmolz + Bickenbach USA Inc..
Journal Articles
Alloy Digest (1984) 33 (8): Ni-301.
Published: 01 August 1984
... Copper 0.01 Chromium 0.001 Aluminum 0.001 Magnesium 0.00 I Nitrogen 0.001 Oxygen 0.02 Nominal Density, lb/cu in. (At 72°F) g/cu cm (At 22°C) Thermal expansion Thermal coef. electrical resistivity / F (72-2 12 F) (72-9320 F) (72-1472 I=) Modulus of elasticity,* psi (At 720F) MPa (At 22oC) Modulus...
Abstract
View articletitled, NICKEL 290: High Purity Nickel
View
PDF
for article titled, NICKEL 290: High Purity Nickel
NICKEL 290 is a high-purity grade of nickel made by a powder-metallurgy process. Its high purity makes it useful for electronic applications such as components of hydrogen thyratrons and for battery applications. The low annealing temperature of Nickel 290 makes it superior to other forms of nickel as a substrate for precious-metal cladding. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-301. Producer or source: Huntington Alloys.
Journal Articles
Alloy Digest (2018) 67 (2): SS-1280.
Published: 01 February 2018
... 0.07 Silicon 0.6 Manganese 1.0 Nickel 4.5 5.5 Chromium 14.5 15.3 Copper 2.5 4.0 Molybdenum 0.5 max Niobium 5×C 0.45 Phosphorus 0.025 Sulfur 0.005 Iron bal Physical Properties Density, 20 °C (68 °F), kg/m3 (lb/in.3) 7800 (0.28) Thermal expansion, 10 6/K (10 6/°F) 20 100 °C (68 212 °F) 10.5 (5.8) 20...
Abstract
View articletitled, UGI 4545 AIR: Precipitation Hardening Martensitic Stainless Steel
View
PDF
for article titled, UGI 4545 AIR: Precipitation Hardening Martensitic Stainless Steel
UGI 4545 Air is a precipitation hardening martensitic stainless steel designed for aerospace applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1280. Producer or source: Schmolz + Bickenbach USA Inc..
Journal Articles
Alloy Digest (1993) 42 (9): Ni-441.
Published: 01 September 1993
..., Wt, %: Chromium Columbium Molybdenum Iron Carbon Aluminum Titanium Cobalt Copper Manganese Nitrogen Phosphorus Silicon Sulfur Nickel 20.0-23.0 3.15-4.15 8.0-10.0 5.0 max. 0.10 max. 0.40 max. 0.40 max. 0.10 max. 0.50 max. 0.50 max. 0.010 max. 0.015 max. 0.50 max. 0.015 max. Balance Table I- MODULUS...
Abstract
View articletitled, CRUCIBLE P/M 625: Corrosion and Oxidation Resistant Nickel-Base <span class="search-highlight">Alloy</span>
View
PDF
for article titled, CRUCIBLE P/M 625: Corrosion and Oxidation Resistant Nickel-Base <span class="search-highlight">Alloy</span>
P/M 625 is a nonmagnetic alloy with outstanding strength and toughness from cryogenic temperatures to 2000 F. It has excellent fatigue strength and stress-corrosion-cracking resistance to chloride ions. This datasheet provides information on composition, microstructureand elasticity as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance. Filing Code: Ni-441. Producer or source: Crucible Compaction Metals.
Journal Articles
Alloy Digest (1999) 48 (6): Ni-554.
Published: 01 June 1999
... is a candidate for critical service industries such as nuclear power, chemical process, pulp, paper, and oil fields. Chemical Composition, wt Chromium 20.0 21.0 Columbium 4.75 5.25 Molybdenum 8.0 9.5 Iron 5.0 max Carbon 0.03 max Aluminum 0.35 0.65 Titanium 0.05 0.30 Cobalt 1.0 max Copper 0.50 max Manganese 0.50...
Abstract
View articletitled, CRUCIBLE P/M 625M: Heat Treatable Nickel-Base CRA
View
PDF
for article titled, CRUCIBLE P/M 625M: Heat Treatable Nickel-Base CRA
Crucible P/M 625M is a powder metallurgy produced alloy where the composition meets both high-strength and corrosion-resistance requirements. P/M 625M is a candidate for critical service industries such as nuclear power, chemical process, pulp, paper, and oil fields. This datasheet provides information on composition, microstructure, and hardness as well as fracture toughness. It also includes information on low temperature performance and corrosion resistance as well as heat treating and powder metal forms. Filing Code: Ni-554. Producer or source: Crucible Compaction Metals.