1-20 of 55 Search Results for

Copper alloy no. 862

Sort by
Journal Articles
Alloy Digest (1979) 28 (1): Cu-365.
Published: 01 January 1979
... Copper Alloy No. 862 is a copper-zinc-aluminum-manganese-iron alloy; aluminum is the principal strengthening element. It is classified as a high-strength yellow brass; its typical tensile strength is 95,000 psi. It has an excellent combination of strength and ductility along with good resistance...
Journal Articles
Alloy Digest (2017) 66 (7): Cu-862.
Published: 01 July 2017
... and bendability in six tempers. For bendability, the r/t values are valid for a strip thickness up to 0.6 mm (0.024 in.) without crack. The Copyright © 2017, ASM International®. All rights reserved. KEMPER KHP®109 (Copper/Tin Alloy) Filing Code: Cu-862 Copper :: July 2017 Materials Park, Ohio 44073-0002...
Journal Articles
Alloy Digest (2000) 49 (4): Cu-618.
Published: 01 April 2000
...% of their stress. ©Copyright 1998, ASM International. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM International Materials Park, Ohio 44073-0002 440-338-5151 Fax 440-338-4634 Mem-Serv@po.ASM-Intl.org WRM ALLOY 5218 Filing Code: Cu-618 Copper June...
Journal Articles
Alloy Digest (2011) 60 (10): Cu-802.
Published: 01 October 2011
... Pfinodal is a copper alloy that is homogenous until cold work and aging occurs, at which point spinodal decomposition increases its strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (2005) 54 (10): Cu-737.
Published: 01 October 2005
... Marinel 230 is an ultrahigh-strength alloy with improved bearing and hardness properties compared to Marinel (see Alloy Digest Cu-602, December 1995). It is a copper alloy with 18% nickel and high manganese and aluminum. It develops high strength with excellent corrosion resistance in seawater...
Journal Articles
Alloy Digest (2002) 51 (8): Cu-687.
Published: 01 August 2002
... CN8) (Hardenable Copper Alloy) Swissmetal alloy SM275H is a hardenable Cu-Ni-Sn alloy with good workability and corrosion resistance. It is often used in the automotive industry for springs, contacts, and clips. Swissmetal is a registered trademark of The Swissmetal Group. Table 1 Mechanical...
Journal Articles
Alloy Digest (1999) 48 (1): Cu-626.
Published: 01 January 1999
... Materials Park, Ohio 44073-0002 440-338-5151 Fax 440-338-4634 Mem-Serv@po.ASM-Intl.org WRM ALLOY 5108 Filing Code: Cu-626 Copper January 1999 Tin 4.8 5.8 Iron 0.05 0.20 Nickel 0.05 0.20 Phosphorus 0.02 0.10 Lead 0.05 max Zinc 0.3 max Copper Balance Copper plus sum of named elements 99.5 min Table 1...
Journal Articles
Alloy Digest (2014) 63 (6): Cu-832.
Published: 01 June 2014
...-338-5151 MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Cu-832 Copper June 2014 BrushForm 158 is a spinodal alloy that develops exceptionally high elastic strength levels, dimensional stability, and relaxation resistance at high temperatures. BRUSHFORM®...
Journal Articles
Alloy Digest (2015) 64 (11): Cu-843.
Published: 01 November 2015
... AM388 is a copper-base spinodal alloy with high strength combined with formability. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on forming and heat treating. Filing Code: Cu-843. Producer...
Journal Articles
Alloy Digest (1994) 43 (10): Al-328.
Published: 01 October 1994
... strength, KS1 (MPa) 30 (207) 0.2% offset yield strength, KS1 (MPa) 24 W9 Elongation in Xhnm (2 in 96 1.5 Corrosion Resistance: Aluminum casting alloys where copper is the major al- loying element are less corrosion-resistant than alloys of other series which contain lower levels of copper. The solution...
Journal Articles
Alloy Digest (2010) 59 (7): Cu-785.
Published: 01 July 2010
... for alloy comparisons. Table 2 Alloy comparisons in tensile strength Tensile strength, MPa (ksi) Ampcoloy 944 820 (119) Beryllium copper (2% Be) 1100 1300 (160 189) Stainless steel 862 1724 (125 250) Tool steel (P20) 900 1000 (131 145) Tool steel (H13) 1420 (206) Ampcoloy 944 is a registered trademark...
Journal Articles
Alloy Digest (2002) 51 (9): SS-862.
Published: 01 September 2002
.... The resulting corrosion will usually be localized to the contact area and may be potentially catastrophic. Datalloy 2 has been designed to counteract this problem and will resist attack even when coupled to pure copper. See Fig. 4. Stress Corrosion. Stress-corrosion cracking (SCC) is caused by the com- bined...
Journal Articles
Alloy Digest (2000) 49 (1): Cu-644.
Published: 01 January 2000
... similar to C52100 but possessing a significantly higher electrical conductivity and improved stress relaxation resistance. The alloy can be used for connectors and contact springs. Chemical Composition, wt Copper 87.0 90.0 Tin 2.5 4.0 Phosphorus 0.02 0.05 Iron 0.05 0.20 Nickel 0.05 0.20 Zinc Balance...
Journal Articles
Alloy Digest (2001) 50 (7): Cu-670.
Published: 01 July 2001
... alloys for bearings capable of performing with a variety of shafting materials and lubricants. ToughMet is a trademark of Brush Wellman, Inc. Chemical Composition, wt (Nominal) Nickel 15 Tin 8 Copper bal Physical Properties: Electrical conductivity, %IACS 9 17 Thermal conductivity, W/m · K (Btu/(ft · h...
Journal Articles
Alloy Digest (1999) 48 (3): Cu-630.
Published: 01 March 1999
...-5151 Fax 440-338-4634 Mem-Serv@po.ASM-Intl.org Filing Code: Cu-630 Copper March 1999 WRM ALLOY 5198 Table 1 Mechanical Properties Standard Relief annealed Tensile strength Yield strength, 0.2% offset Elongation in Tensile strength Yield strength, 0.2% offset Elongation in Temper MPa ksi MPa ksi 51 mm...
Journal Articles
Alloy Digest (2014) 63 (7): Cu-833.
Published: 01 July 2014
... BrushForm 96 strip is a high-performance, heat treatable spinodal copper-nickel-tin alloy designed to provide optimal formability and strength characteristics in conductive spring applications. It is available in both pre-heat treated (mill hardened) and heat treatable (age hardenable) forms...
Journal Articles
Alloy Digest (2009) 58 (3): Cu-767.
Published: 01 March 2009
..., ¼ hard 552 80 331 48 20 H02, ½ hard 676 98 393 57 8 H04, hard 862 125 448 65 5 H08, spring 1000 145 483 70 3 DATA ON WORLDWIDE METALS AND ALLOYS Filing Code: Cu-767 Copper March 2009 Copyright © 2009, ASM International®. All rights reserved. Data shown are typical, not to be used for specification...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-636.
Published: 01 October 1999
... ALLOY 5118 (Modified Phosphor Bronze Alloy) WRM alloy 5118 is a modified phosphor bronze alloy that exhibits improved strength while maintaining good stress-relaxation characteristics. The patent is pending. Chemical Composition, wt Copper Balance Tin 3.5 4.9 Iron 0.05 0.20 Nickel 0.11 0.20 Phosphorus...
Journal Articles
Alloy Digest (2000) 49 (1): Cu-645.
Published: 01 January 2000
... after forming. There is no increase in stress-corrosion susceptibility as a result of this treatment. Corrosion Resistance: Olin C688 shares the resistance to general corrosion common to most copper alloys. Because of its aluminum content, how- ever, it is more resistant to tarnishing than other alloys...
Journal Articles
Alloy Digest (2004) 53 (6): Al-389.
Published: 01 June 2004
... General Characteristics: 2524 is a heat treatable aluminum-copper alloy offering high toughness and improved resistance to fatigue crack growth rela- tive to other available 2xxx sheet and plate materials. Fatigue crack growth improvements are guaranteed through the material specification for Alclad 2524...