Alloy Digest (1978) 27 (3): Cu-349.
Published: 01 March 1978
... Copper Alloy No. 844 is a free-cutting copper-tin-lead-zinc alloy for castings; it was formerly identified as 81-3-7-9 alloy. It is characterized by good casting properties, moderate strength and ductility, good machinability and good resistance to corrosion. It is used widely for fittings...
Journal Articles
Alloy Digest (1997) 46 (3): Cu-611.
Published: 01 March 1997
... & Fressure tightness: Exceptional Corrosion resistance: Good Polishing, buffing. or plating: Good Corrosion Resistance: Leachate concentration (potable water): extremely low Specification Equivalents: Copper Alloy No. C8983 1 DOI: 10.31399/asm.ad.cu0611 General Characteristics: The basis for developing lead...
Journal Articles
Alloy Digest (2015) 64 (11): Cu-844.
Published: 01 November 2015
... Alloy) Filing Code: Cu-844 Copper :: November 2015 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.8542 :: www.asminternational.org :: MemberServiceCenter@asminternational.org Published by ASM International® :: Data shown are typical, not to be used for specification or final design...
Journal Articles
Alloy Digest (2019) 68 (7): Cu-891.
Published: 01 July 2019
...) 355 (0.085) Melting point liquidus, °C (°F) 1025 (1877) Melting point solidus, °C (°F) 790 (1454) Electrical Conductivity. IACS = International Annealed Copper Standard; depending on temper Copyright © 2019, ASM International®. All rights reserved. CONCAST C89833 (Copper Casting Alloy) Filing Code...
Journal Articles
Alloy Digest (2002) 51 (2): SS-844.
Published: 01 February 2002
.../asm.ad.ss0844 the base metal for as-welded structures. AWS 5.11/5.14 materials E/ER NiCrMo-3, 10, or 13 are often recommended for this reason. Specification Equivalents: UNS N08904 ASTM B 625 General Characteristics: Carlson alloy 904L is an austenitic nickel-chromium stainless steel with molybdenum and copper...
Journal Articles
Alloy Digest (2013) 62 (3): SS-1138.
Published: 01 March 2013
... NITRONIC 30® Chemical Composition, wt (Maximum) Carbon 0.03 Manganese 7.0 9.0 Phosphorus 0.040 Sulfur 0.030 Silicon 1.00 Chromium 15.0 17.0 Nickel 1.5 3.0 Nitrogen 0.15 0.30 Copper 1.00 Iron bal Physical Properties: Density, 21 °C (70 °F), kg/m3 (lb/in.3) 7862 (0.283) Mechanical Properties: Modulus...
Journal Articles
Alloy Digest (2020) 69 (1): SS-1314.
Published: 01 January 2020
... and stamped automotive trim applications. Chemical Composition Composition, wt%(a) Element Types 430, 434, and 436 Type 435 Mod Carbon 0.12 0.020 Silicon 1.00 1.00 Manganese 1.00 1.00 Phosphorus 0.040 0.040 Sulfur 0.030 0.012 Chromium 16.0 18.0 19.0 21.0 Molybdenum (b) Nickel (c) 0.60 Copper 0.30 0.60...