Alloy Digest (1976) 25 (8): Cu-317.
Published: 01 August 1976
... Copper Alloy No. 836 is a free-cutting copper-tin-lead-zinc alloy for castings. It offers good casting characteristics, moderate strength and ductility, good machinability and good resistance to corrosion. It is used widely for such applications as valves, gears and general hardware. This...
Journal Articles
Alloy Digest (1997) 46 (4): Cu-612.
Published: 01 April 1997
... and mechanical proper- ties: small Patternmakers shrinkage (inJft): I,& pressun tighIness: Exceptional Corrosion msistance: Good Polishing. buffing, or plating: Good Corrosion Resistance: Leachate concentration (potable water): Extremely low Specification Equivalents: Copper Alloy No. C89833 General...
Journal Articles
Alloy Digest (1974) 23 (6): Cu-279.
Published: 01 June 1974
... alloy. It has excellent resistance to dezincification which makes it highly suit- able for water-system applications, decorative parts and marine fittings. *U.S. Patent No. 3,713,814 assigned to Olof Manner AB. Composition: Copper Tin Lead Aluminum Iron Manganese Nickel Antimony Silicon zinc Nominal...
Journal Articles
Alloy Digest (1978) 27 (12): Cu-364.
Published: 01 December 1978
... sulfuric acid and most weak acids. It is highly resistant to steam. It is very resistant to dezinc- ification, and therefore, makes an excellent alloy for valve stems for water and high pressure steam valves. Specification Equivalents: ASTM B 37 1 (Copper Alloy No. 697). CDA Alloy No. 697. UNS No. C69700...
Journal Articles
Alloy Digest (1995) 44 (12): Ni-494.
Published: 01 December 1995
.... eNimofer ia a registered irakmrk of KRUPP-VDM GmbH Chemical comPoeltlon WL, %: Maw== silicorl Nickel chromillm copper Phosphorus StllflU Molybdenum CQbalt MitL 0.3 1.0 26.0 Max. 0.01 1.0 0.08 Balance 1.0 0.5 0.02 0.010 20 30.0 1.0 Physical Properties: Density, lb/cu in. (g/cu cm) Melting range, F ( C...