Journal Articles
Alloy Digest (1979) 28 (4): Cu-370.
Published: 01 April 1979
... castability chemical composition Copper alloy no. 803 corrosion-resistant alloys ductility elasticity electrical conductivity fatigue properties hardness heat treatability joinability machinability physical properties tensile properties thermal conductivity Copper No, 803 Filing Code: cu-370...
Journal Articles
Alloy Digest (2012) 61 (2): Cu-803.
Published: 01 February 2012
... PCLW-SNX alloy is a copper-base negative extension wire used instead of platinum as a compensating leg in Type S and R thermocouples. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming. Filing Code: Cu-803...
Journal Articles
Alloy Digest (1955) 4 (9): Cu-31.
Published: 01 September 1955
... composition corrosion-resistant alloys elasticity hardness joinability machinability MUELLER 803 physical properties tensile properties workability I I Filing Code: Cu-31 MUELLER 803 Copper Alloy SEPTEMBER 1955 DIGEST d - DATA ON WORLD WIDE METALS AND ALLOYS Pnblisbd by hgkaing Alloys Dig&r, Inc...
Journal Articles
Alloy Digest (1993) 42 (12): SS-559.
Published: 01 December 1993
...-, and/or sulfidation-resistance are important @INCOLOY is a trademark of the Into family of companies Chemical Composition, Wt., %: Nickel 32-37 Chromium 25-29 Carbon 0.06-0.10 Manganese 1.5 max. sulfur 0.015 max. Silicon 1.0 max. Copper 0.75 max. Aluminum 0.15-0.60 Titanium 0.15-0.60 Iron Balance Physical Properties...
Journal Articles
Alloy Digest (2003) 52 (8): Ni-611.
Published: 01 August 2003
... joinability physical properties tensile properties workability thermal properties UNS N08890 Chemical Composition, wt (Nominal) Nickel 42.5 Chromium 25 Aluminum 0.1 Niobium 0.4 Titanium 1 max Carbon 0.1 Manganese 1 max Silicon 1.8 Phosphorous 0.03 max Sulfur 0.015 max Copper 0.75 max Molybdenum 1.5...
Journal Articles
Alloy Digest (2015) 64 (10): Cu-842.
Published: 01 October 2015
... Carpenter PCLW-BPX alloy is a copper-base positive extension wire used with copper. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming. Filing Code: Cu-842. Producer or source: Carpenter Specialty Wire Products...
Journal Articles
Alloy Digest (1991) 40 (10): Cu-565.
Published: 01 October 1991
... Copper Alloy No. C43500 is a tin containing brass. It has strength and ductility comparable to low brass (80% copper, 20% zinc). It has excellent cold workability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...
Journal Articles
Alloy Digest (1994) 43 (11): Cu-599.
Published: 01 November 1994
... COPPER ALLOY NOS. C44400 and C44500 are copper-zinc-tin alloys inhibited by antimony and phosphorus, respectively. They are commonly known as inhibited admiralty metal or admiralty brass. They have a good combination of strength and ductility and good resistance to general corrosion. The small...
Journal Articles
Alloy Digest (2017) 66 (10): SA-803.
Published: 01 October 2017
... 0.030 max Sulfur 0.030 max Chromium 0.40 0.65 Copper 0.25 0.40 Nickel 0.40 max Vanadium 0.02 0.10 Iron bal In order to obtain fine-grain structure a sufficient amount of nitrogen absorbing elements is added (e.g., . 0.02% Al). Mechanical Properties: Minimum yield strength, ReH, MPa (ksi) 16 mm (0.6...
Journal Articles
Alloy Digest (2007) 56 (12): Ti-144.
Published: 01 December 2007
... tensile properties TIMETAL 230 workability thermal properties UNS R56260 Chemical Composition, wt Copper 2.00 3.00 Iron 0.20 max Oxygen 0.20 max Carbon 0.08 max Nitrogen 0.03 max Hydrogen 0.01 max Residual elements, each 0.10 max Residual elements, total 0.40 max Titanium bal TIMETAL® 230 Filing...
Journal Articles
Alloy Digest (2005) 54 (2): SS-917.
Published: 01 February 2005
... properties tensile properties thermal properties Chemical Composition, wt (Typical, except where otherwise noted) Nickel 8.75 15.5 Chromium 19.5 21.0 Molybdenum 0.4 Aluminum 0.15 Manganese 0.4 Titanium 0.4 Copper 0.75 max Silicon 0.7 Carbon 0.05 max Sulfur 0.005 max Iron bal Physical Properties: Density...
Journal Articles
Alloy Digest (2011) 60 (3): Al-436.
Published: 01 March 2011
..., rod, bar, and profiles. This alloy has good corrosion resistance, good weldability, and a good anodizing response. KAISER ALLOY 6063 (High Strength Extruded and Drawn Products) KAISER ALLOY 6063 Chemical Composition, wt (Nominal) Silicon 0.20 0.6 Iron 0.35 max Copper 0.1 max Manganese 0.1 max...
Journal Articles
Alloy Digest (1995) 44 (2): Ni-477.
Published: 01 February 1995
... with chromium, silicon, and rare earth additions to produce an alloy oxidation resistant, especially for applications such as waste incineration. NICROFER@ is a registered trademark of KRUPP-VDM GmbH. Composition, Wt. %: Physical Properties: Carbon h4anganese Silicon Nickel Chromium Copper Iron Rare Earth...
Journal Articles
Alloy Digest (2017) 66 (11): SA-805.
Published: 01 November 2017
... chemical composition, when utilized unprotected, exhibits resistance to atmospheric corrosion over unalloyed steels. Chemical Composition, wt Carbon 0.12 max Silicon 0.25 0.75 Manganese 0.20 0.50 Phosphorus 0.07 0.15 Sulfur 0.030 max Chromium 0.50 1.25 Copper 0.25 0.55 Nickel 0.65 max Iron bal In order...
Journal Articles
Alloy Digest (2021) 70 (11): Ni-777.
Published: 01 November 2021
..., velocity, crevices, deposits, metallurgical Nickel condition, stress, surface finish, and dissimilar metal contact. Chromium bal 44.5 min Cobalt Molybdenum 20.0 24.0 20.0 24.0 Iron Manganese 10.0 15.0 10.0 15.0 Aluminum Carbon 8.0 10.0 8.0 10.0 Environment Rating Environment Rating Copper Acetic acid...
Journal Articles
Alloy Digest (2016) 65 (1): SS-1235.
Published: 01 January 2016
... 0.015 Silicon 1.00 Chromium 19.5 21.5 Nickel 8.0 9.5 Molybdenum 0.5 1.50 Copper 1.00 Nitrogen 0.14 0.25 Iron bal Physical Properties: Density, kg/m3 (lb/in.3) 7870 (0.283) Thermal conductivity, W/m·K (Btu/(h·ft·°F)) 13.8 (8.0) Heat capacity, J/kg·K (Btu/lb·°F) 470 (0.112) Magnetizable No For linear...
Journal Articles
Alloy Digest (1981) 30 (4): Ni-267.
Published: 01 April 1981
... as possible by using copper back-up bars and water cooled futures. Good joint fit-up is necessary to minimize the tendency for cracking when highly restrained. When tiller material is desired, either Unitemp 41, Hastelloy W or Into-Weld A or other proven materials may be used. The literature contains useful...