Journal Articles
Alloy Digest (1975) 24 (1): Cu-290.
Published: 01 January 1975
... Copper Alloy No. 735 (Also called Nickel Silver 72-18) has excellent ductility and excellent resistance to corrosion. It is darkest in color of all the nickel silvers. Its applications include fishing reels and watch parts. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2013) 62 (12): Cu-828.
Published: 01 December 2013
... rod extensions for resistance seam and spot welding. Producer: Ansonia Copper & Brass, Inc. Ansonia, CT 06401, USA Tel: (800) 521-1703 Fax: (203) 735-3787 www.ansoniacb.com ISSN: 002-614X Cu-828B ...
Journal Articles
Alloy Digest (2008) 57 (3): Cu-752.
Published: 01 March 2008
... C14500 answers fabrication problems that no other alloy has so satisfactorily solved. Its mechanical properties are similar to that of unalloyed, pure copper, yet its machinability rating of 85% is considerably higher by 20% over unalloyed coppers. This alloy thus possesses a unique combination of...
Journal Articles
Alloy Digest (1998) 47 (12): SS-735.
Published: 01 December 1998
... S31603 - DIGEST - riltism DATA ON WORLD WIDE METALS AND ALLOYS w 19iW, ASM lntematma 1. All rights reserwdDataahownare&pical,nottok usedtors+aecaationor~design. Filing Code S-735 m StainlessStd mmber 1998 PublishedtyASMlnte~ Materlals Park, otuo 44073anl? 440-238-5151 Faxalxm463 A.4C?m-.SRVB~.ASM-l...
Journal Articles
Alloy Digest (2011) 60 (5): Cu-798.
Published: 01 May 2011
... carriers, and are subject to torque stresses. Using this alloy gives them the high resistant to torque while allowing them to be tightly mounted for maximum heat transfer. Producer: Ansonia Copper & Brass, Inc. Waterbury, CT, 06708 USA Phone: (800) 512-1703 or (203) 735-3787 www.ansoniacb.com ISSN: 002...
Journal Articles
Alloy Digest (1982) 31 (5): SS-407.
Published: 01 May 1982
..., recuperators. combustion chambers. soot blowers, neutral salt-pot electrodes, oil-burner components, spouts for conveying molten copper alloys. kiln linings, thermo- couple protection tubes, stack dampers, boiler baffles, gas-injec- tion nozzles for various molten compounds and flame rods. Manufacturers...
Journal Articles
Alloy Digest (2015) 64 (12): SS-1234.
Published: 01 December 2015
... properties workability UNS N08925 NSSMC-NAR-AC-3 and AC-4 are austenitic stainless steels with excellent corrosion resistance, especially to seawater. Chemical Composition, wt (Typical) AC-3 AC-4 Chromium 20.0 23.0 Nitrogen 0.14 0.25 Molybdenum 6.2 6.1 Carbon 0.02 max 0.03 max Copper 1.0 Nickel 25.0...