Skip Nav Destination
Close Modal
Search Results for
Copper alloy no. 505
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 85 Search Results for
Copper alloy no. 505
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1974) 23 (9): Cu-285.
Published: 01 September 1974
... Copper Alloy No. 505 is a 1.25% tin-phosphorus bronze with good tensile and yield strengths and good resistance to corrosion and fatigue. It is recommended for flexible hose and electrical contacts and conductors. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
Copper Alloy No. 505 is a 1.25% tin-phosphorus bronze with good tensile and yield strengths and good resistance to corrosion and fatigue. It is recommended for flexible hose and electrical contacts and conductors. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-285. Producer or source: Copper and copper alloy mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (2): Ni-215.
Published: 01 February 1975
... Nickel-Copper Alloys 505 and 506 are strong castings alloys. Both alloys combine high strength with good wear resistance. Alloy 505 (4% silicon) is employed where exceptional resistance to galling is needed. Alloy 506 (3% silicon) is recommended where good (but not exceptional) galling resistance...
Abstract
View article
PDF
Nickel-Copper Alloys 505 and 506 are strong castings alloys. Both alloys combine high strength with good wear resistance. Alloy 505 (4% silicon) is employed where exceptional resistance to galling is needed. Alloy 506 (3% silicon) is recommended where good (but not exceptional) galling resistance is sufficient. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion and wear resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Ni-215. Producer or source: Nickel alloy casting producers.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (1): Cu-505.
Published: 01 January 1986
... 290 Filing Code: Cu-505 Olr Copper Alloy JANUARY 1986 BIGHT - DATA ON WORLD WIDE METALS AND AUOYS Putdished /P,I 0 Copyright 1985. Alloy Digest. Inc All nghlr rexned ISSN3LG614X Alloy Digest. Inc. 27 Canlield Street Orange. New Jersey 07050 (201) 761-1090 BRUSHFORM 290 (Beryllium-Copper Alloy...
Abstract
View article
PDF
BRUSHFORM 290 is a specially processed, mill-hardened beryllium copper alloy having improved formability while maintaining the strength of other mill-hardened copper beryllium alloys. It was developed for current carrying springs requiring greater formability. It can be used in a number of applications formerly limited to heat treatable tempers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming and heat treating. Filing Code: Cu-505. Producer or source: Brush Wellman Inc.. See also Alloy Digest Cu-650, July 2000.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (12): Cu-385.
Published: 01 December 1979
... joinability machinability metal hose physical properties tensile properties thermal conductivity workability wrought bronze UNS C50500 All Filing Code: Cu-385 ANACONDA Alloy (k) 505 Copper Alloy @r DECEMBER 1979 BICIST - DATA ON WORLD WIDE METALS AND ALLOYS lbgyT$zy>gs Inc. Upper Mmtclair. New...
Abstract
View article
PDF
ANACONDA Alloy (E) 505 is a low-tin phosphor bronze with excellent resistance to corrosion, excellent ductility and good resistance to fatigue. It has good thermal and electrical conductivity. Its uses include flexible metal hose, electrical contacts, fuse clips and fasteners. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-385. Producer or source: Anaconda American Brass Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1962) 11 (8): Ni-73.
Published: 01 August 1962
... MONEL alloy 506 is an intermediate cast nickel-copper alloy that has higher hardness than cast Monel alloy 410 and better machinability than Monel alloy 505. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Abstract
View article
PDF
MONEL alloy 506 is an intermediate cast nickel-copper alloy that has higher hardness than cast Monel alloy 410 and better machinability than Monel alloy 505. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Ni-73. Producer or source: Huntington Alloy Products Division.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (7): Cu-650.
Published: 01 July 2000
... Brushform 290 is a high-strength beryllium-copper alloy used in electronic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming...
Abstract
View article
PDF
Brushform 290 is a high-strength beryllium-copper alloy used in electronic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming. Filing Code: CU-650. Producer or source: Brush Wellman Inc. See also Alloy Digest Cu-505, January 1986.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (5): Cu-477.
Published: 01 May 1984
...-cast bars. Values are those specified in ASTM B 505) Tensile strength. psi (MPa), min Yield strength (0.5yc extension psi (MPa), min Elongation (2 in. or 50 mm). q# *Under load. 38000 (252) 20000 ( 138) 8 DOI: 10.31399/asm.ad.cu0477 Copyright © ASM International® 1996 Heat Treatment: Copper Alloy...
Abstract
View article
PDF
Copper Alloy No. C92700 is a cast copper-base alloy; it formerly was known as 88-10-2-0 alloy. It is characterized by a good combination of machinability, strength and resistance to corrosion. Among its many uses are bearings, pump impellers, piston rings and valve parts that are subject to liquid and or gas pressure and, therefore, must be sound (free from defects). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-477. Producer or source: Copper alloy foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (6): Cu-355.
Published: 01 June 1978
... with varying degrees of severity if moisture is present in these gases. Specification Equivalents: ASTM: B 30, B 271, B 505, B 584 (formerly B 143). SAE: J 461 and J 462. Military: MIL-C-15345, Alloy 10. Federal: QQ-C-390. Ingot No. 230. General Characteristics: Copper Alloy No. 923 is nominally an 87% copper...
Abstract
View article
PDF
Copper Alloy No. 923 is a cast copper-tin-zinc-lead alloy known also as Leaded G Bronze or 87-8-1-4 alloy. This alloy possesses a good combination of strength, resistance to corrosion and machinability. It is a good alloy to withstand gas or liquid pressures. Applications include pump impellers, fittings and bearings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-355. Producer or source: Copper alloy foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (12): Cu-345.
Published: 01 December 1977
... Copper Alloy No. 903 is a cast copper-tin-zinc alloy known also as G Bronze or 88-8-0-4 alloy. It has a good combination of strength and corrosion resistance and is often used in castings subject to liquid or gas pressures. Among its many uses are valves, pumps, bushings and gears. This datasheet...
Abstract
View article
PDF
Copper Alloy No. 903 is a cast copper-tin-zinc alloy known also as G Bronze or 88-8-0-4 alloy. It has a good combination of strength and corrosion resistance and is often used in castings subject to liquid or gas pressures. Among its many uses are valves, pumps, bushings and gears. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-345. Producer or source: Copper alloy foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (12): Cu-450.
Published: 01 December 1982
... Equivalents: ASTM: B 30 and B 505. Federal: QQ-C-390. Ingot No. 101. UNS No. C84200. General Characteristics: The composition of Copper Alloy No. C84200 is nominally 80% copper, 5% tin, 2.5% lead and 12.5% zinc. It can be produced as centrifugal castings, con- tinuous castings and sand castings. It has good...
Abstract
View article
PDF
Copper Alloy No.1 C84200 is a free-machining copper-tin-lead-zinc alloy for castings; it was formerly identified as 80-5-2.5-12.5 alloy. It has good casting characteristics, good machinability, moderate strength and ductility and good corrosion resistance. Among its many uses are ornamental fixtures, general hardware, plumbing goods, small gears and pipe fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-450. Producer or source: Copper alloy foundries. See also Alloy Digest Cu-446, October 1982.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (4): Cu-475.
Published: 01 April 1984
... Copper Alloy No. C93900 is a cast copper-tin-lead alloy (bronze). It has good machinability, low strength and good resistance to corrosion. This alloy formerly was known by several commercial names (not recommended); they are: (1) High-Leaded Tin Bronze and (2) 79-6-15. It is produced only...
Abstract
View article
PDF
Copper Alloy No. C93900 is a cast copper-tin-lead alloy (bronze). It has good machinability, low strength and good resistance to corrosion. This alloy formerly was known by several commercial names (not recommended); they are: (1) High-Leaded Tin Bronze and (2) 79-6-15. It is produced only in the form of continuous castings and its uses include bearings, pump bodies and impellers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-475. Producer or source: Copper alloy foundries. See also Alloy Digest Cu-487, November 1984.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (2): Cu-432.
Published: 01 February 1982
... in these gases. Specification Equivalents: ASTM: B 22, B 30, B 271, B 505 and B 584 (formerly B 143). AMS 4845. SAE: 5461 and J462. Federal QQC-390. Ingot No. 210. General Characteristics: Copper Alloy No. C90500 is nominally an 88% copper- 10% tin-2% zinc casting alloy. The tin and zinc greatly increase its...
Abstract
View article
PDF
Copper Alloy no. C90500 is a cast copper-tin-zinc alloy known also by names formerly used (not recommended): Gun Metal, 210, Tin Bronze and 88-10-0-2. It has a good combination of strength and resistance to corrosion. Because of its mechanical properties and corrosion resistance, it is used frequently in castings that are subjected to liquid or gas pressure, such as those in valves, pumps, etc. It also is used for bearings and gears. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-432. Producer or source: Copper alloy foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (10): Cu-382.
Published: 01 October 1979
... in ASTM B 505) Tensile strength, mm, psi (MPa) 38000 (262) Yield strength (0.5% extension min, psi (MPa) 19000 (131) Elongation (2 in.; 50.8 mm), % 18 *Under load. DOI: 10.31399/asm.ad.cu0382 Copyright © ASM International® 1996 Heat Treatment: Copper Alloy No. 922 is used in the as-cast condition...
Abstract
View article
PDF
Copper Alloy No. 922 is a cast copper-tin-zinc-lead alloy formerly identified as Navy M or 88-6-1.5-4.5 alloy. It possesses a good combination of machinability, strength and resistance to corrosion. Alloy No. 922 is a good material to use in castings subject to liquid or gas pressures. Its many uses include valves, piston rings and pump impellers. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-382. Producer or source: Copper alloy foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (11): Cu-487.
Published: 01 November 1984
... Copper Alloy No. C93900 is a cast bronze of fairly low strength. It has good machinability and good resistance to corrosion. Its commercial names formerly used (not recommended) are: (1) High-Leaded Tin Bronze and (2) 79-6-15. Among its uses are bearings for general service and pump bodies...
Abstract
View article
PDF
Copper Alloy No. C93900 is a cast bronze of fairly low strength. It has good machinability and good resistance to corrosion. Its commercial names formerly used (not recommended) are: (1) High-Leaded Tin Bronze and (2) 79-6-15. Among its uses are bearings for general service and pump bodies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-487. Producer or source: Copper alloy foundries. See also Alloy Digest Cu-475, April 1984.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (6): Cu-439.
Published: 01 June 1982
... contact with mercury com- pounds, oxidizing acids, cyanides, moist ammonia and strong bases. Specification Equivalents: ASTM: B 30, B 271, B 505 and B 584. Federal: QQ-C-390. SAE: J 461 and J 462. Ingot No. 326. CDA No. C93500. UNS No. C93500. General Characteristics: Copper Alloy No. C93500 is a copper...
Abstract
View article
PDF
Copper Alloy No. C93500 is a cast bronze containing nominally 9% lead and 5% tin. It has excellent machinability, low strength and good resistance to corrosion. It is used for corrosion-resistant castings, small bearings and bushings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-439. Producer or source: Copper alloy foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (6): Cu-460.
Published: 01 June 1983
... to carbon dioxide, sulfur dioxide, and sulfur trioxide even in the presence of moisture. Specifkation Equivalents: ASTM: B 30, B 427 and B 505. SAE J 461 and J 462 Ingot No. 205. UNS No. C9O7OO. General Characteristics: Copper Alloy No. C9O7OO is nominally an 8% copper, 11% tin casting alloy that has been...
Abstract
View article
PDF
Copper Alloy No. C90700 is a cast copper-tin alloy known also by names formerly used (but not recommended): Tin Bronze, 205 and 89-11. It is a medium-strength alloy and has a good combination of strength, ductility and resistance to corrosion. Among its many uses are gears, bearings, bushings and marine hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-460. Producer or source: Copper alloy foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (10): Cu-446.
Published: 01 October 1982
... and strong bases should be avoided. Specification Equivalents: UNS No. C84200. QQ-C-390. ASTM: B 30 and B 505. Ingot No. 101. General Characteristics: Copper Alloy No. C84200 contains nominally 80% copper, 12.5% zinc, 5% tin and 2.5% lead. Sand molding is the most common eating method; also, centrifugal...
Abstract
View article
PDF
Copper Alloy No. C84200 is a free-cutting copper-zinc-tin-lead alloy. It is characterized by good casting properties, moderate strength and ductility, good machinability and good resistance to corrosion. Formerly used named (not recommended) are 101, Leaded Semi-Red Brass and 80-5-2.5-12.5. Typical applications are pipe fittings, bushings, locknuts and unions. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-446. Producer or source: Copper alloy foundries. See also Alloy Digest Cu-450, December 1982.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (1): Cu-470.
Published: 01 January 1984
..., moist ammonia and strong bases. Specification Equivalents: ASTM:B 30, B 66, B 271, B 505 and B 584 (formerly B 144). Federal: QQC-390 (Alloy 18). Military: MIL-B- 16261 (Alloy V). Ingot No. 322. SAE: 5462 (CA943). UNS No. 04300. General Characteristics: Copper Alloy No. C94300 is a high-leaded bronze...
Abstract
View article
PDF
Copper Alloy No. C94300 is a cast copper-tin-lead alloy (bronze). It is characterized by low hardness and strength, medium ductility, excellent machinability and good resistance to corrosion. Commercial names formerly used (but not recommended) are (1) Ingot No. 322, (2) Soft Bronze, (3) High-Leaded Tin Bronze and (4) 70-5-25. This alloy is recommended highly for high-speed bearings at light loads. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-470. Producer or source: Copper alloy foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (10): Cu-464.
Published: 01 October 1983
... Copper Alloy No. C93800 is a cast copper-tin-lead alloy (bronze). It is characterized by low strength, good machinability and good resistance to corrosion. Commercial names formerly used (not recommended) are (1) Anti-Acid Metal, (2) Ingot No. 319, (3) High-Leaded Tin Bronze and (4) 78-7-15. Its...
Abstract
View article
PDF
Copper Alloy No. C93800 is a cast copper-tin-lead alloy (bronze). It is characterized by low strength, good machinability and good resistance to corrosion. Commercial names formerly used (not recommended) are (1) Anti-Acid Metal, (2) Ingot No. 319, (3) High-Leaded Tin Bronze and (4) 78-7-15. Its many applications include bearings, bushings, pump impellers and corrosion-resistant castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-464. Producer or source: Copper alloy foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (1): Cu-387.
Published: 01 January 1980
... Copper Alloy No. 932 is a cast bronze containing nominally 7% lead and 7% tin. Commercial names formerly used (not recommended) are (1) High-Leaded Tin Bronze, (2) Bearing Bronze 660 and 83-7-7-3. It has relatively low strength, good machinability and good resistance to corrosion. Its uses include...
Abstract
View article
PDF
Copper Alloy No. 932 is a cast bronze containing nominally 7% lead and 7% tin. Commercial names formerly used (not recommended) are (1) High-Leaded Tin Bronze, (2) Bearing Bronze 660 and 83-7-7-3. It has relatively low strength, good machinability and good resistance to corrosion. Its uses include bushings, bearings and corrosion-resistant castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-387. Producer or source: Copper alloy foundries.