Alloy Digest (1974) 23 (6): Cu-280.
Published: 01 June 1974
... COPPER Alloy No. 425 is a copper-zinc-tin alloy suitable for electrical switches and springs, fuse and pen clips, and weather stripping. It can be cold worked readily by convectional processes. This datasheet provides information on composition, physical properties, hardness, elasticity, and...
Journal Articles
Alloy Digest (1987) 36 (10): Cu-529.
Published: 01 October 1987
... Copper Alloy No. C68800 is a wrought copper-base alloy (modified brass) containing nominally 22.7% zinc, 3.4% aluminum and 0.40% cobalt. It has high strength and fairly good ductility. It can be hardened and strengthened further by heating temper-rolled material to 425 F where an ordering reaction...
Journal Articles
Alloy Digest (1993) 42 (5): Cu-583.
Published: 01 May 1993
... Copper No. C15710 is a dispersion strengthened alloy with alumina. The strength is higher than copper while maintaining good electrical properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on...
Journal Articles
Alloy Digest (1994) 43 (12): Cu-540.
Published: 01 December 1994
... COPPER ALLOY NO. C15500 is a silver-bearing copper alloy with softening resistance. A typical application is lead frames for electric devices. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1976) 25 (5): Cu-312.
Published: 01 May 1976
... Copyright © ASM International® 1996 1996 ASM International bearings chemical composition collector rings Copper No. 150 corrosion-resistant alloys creep properties current carrying shafts ductility elasticity hardness heat treatability joinability machinability physical properties...
Journal Articles
Alloy Digest (1990) 39 (12): Cu-556.
Published: 01 December 1990
... International® 1996DOI: 10.31399/asm.ad.ts0498 Heat Treatment: Copper alloy No. C32000 is not hardenable by heat treat- ment. It may be annealed at 800-1200°F (425-650 (Z). Machinability: Copper alloy No. C32000 is readily machinable, having a rating of 90 on a scale where free-cutting brass is rated 100. It is...
Journal Articles
Alloy Digest (1991) 40 (5): Cu-560.
Published: 01 May 1991
... Temper ksi ksi (;I Hardness 0.025mm grain size 56.0 23.0 50.0 82F Harddrawn 74.0 55.0 10.0 80B Copyright © ASM International® 1996DOI: 10.31399/asm.ad.cu0560 Heat Treatment : Copper Alloy No. C27400 is not hardenable by heat treatment. Anneal at 800- 1300°F (425-700°C). Machinability: Machinability...
Journal Articles
Alloy Digest (1989) 38 (7): Cu-548.
Published: 01 July 1989
.... diameter minimum section specimens on 1/2Hard( lS%CR) bar had fatigue strengths of 14 and 20 ksi. Copyright © ASM International® 1996DOI: 10.31399/asm.ad.cu0548 Heat Treatment: Copper Alloy No. C36000 is not hardenable by heat treatment. To anneal the alloy, heat to 800-l 100°F (425- 600°C); cool at any...
Journal Articles
Alloy Digest (1994) 43 (11): Cu-599.
Published: 01 November 1994
...% 0.10% 1 .OOz 205 (400) 13cuKl(90) 17000 (117) 19ooo (130) 315 (600) 1000 (6.9) 1950 (13.4) 3800 (26) 425 (800) 54 (0.37) 160 (1.1) 500 (3.4) Heat Treatment: Annealing: Heat Copper Alloy Nos. C44400 and C44500 to 800- llW Fandcoolatanydesiredmte.Thetempcranrrcandtimcat tenpxatme will depend on the...
Journal Articles
Alloy Digest (1984) 33 (5): Cu-476.
Published: 01 May 1984
... Copper Alloy No. C34200 contains nominally 2% lead and has a machinability rating approaching that of Free-Cutting Brass. It is noted for its excellent thread-rolling and knurling properties. It is used for many screw-machine applications and it has good resistance to corrosion in many...
Journal Articles
Alloy Digest (1985) 34 (2): Cu-492.
Published: 01 February 1985
... aluminum bronze. It has moderate strength and ductility, good toughness and good resistance to shock. It maintains its mechanical properties at low temperatures and to about 425 F. Its impact and fatigue properties are good. Copper Alloy No. C61800 has good hot-working characteristics and fair cold...
Journal Articles
Alloy Digest (1987) 36 (7): Cu-526.
Published: 01 July 1987
... Copper Alloy No. C44300 is a copper-zinc-tin alloy inhibited by arsenic; it is commonly known as inhibited admiralty metal or admiralty brass. It has a good combination of strength and ductility and good resistance to general corrosion. The small addition of arsenic (nominally 0.06%) is made to...
Journal Articles
Alloy Digest (1981) 30 (4): Cu-415.
Published: 01 April 1981
...-1200°F (425-65OOC) and cooled at any desired rate. Stress Relieving: Heat this alloy to 450-6OOoF (230- 3150C) and cool at any desired rate. This treatment may be desirable in some instances to relieve machin- ing stresses. Hardening: Copper Alloy No. C34000 cannot be hard- ened or strengthened by any...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-620.
Published: 01 October 1999
... WRM Alloy 194-9 is a modified C19400 with mechanical properties far exceeding the conventional composition (see COPPER ALLOY No. 194, Alloy Digest Cu-233, May 1971). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (2013) 62 (6): Cu-820.
Published: 01 June 2013
... MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Copper June 2013 Cu-820 Mueller Alloy C27450 has excellent machining characteristics for forged and machined applications required to meet AB1953. MUELLER ALLOY C27450 (No Lead Plumbing Brass) MUELLER ALLOY C27450 Chemical...
Journal Articles
Alloy Digest (1985) 34 (6): Cu-497.
Published: 01 June 1985
... stress- relieving treatment should be used. Specification Equivalents: ASTM: B I I 1, B I7 1, B 359. B 395, B 432 and B 543. ASME: SBl I I. SB171, SB 359. SB395 and SB543. UNS No. C44300. General Characteristics: Mueller Alloy 4430 is a copper-zinc-tin alloy inhibited by a small addition of arsenic...
Journal Articles
Alloy Digest (2013) 62 (12): Cu-828.
Published: 01 December 2013
... Ansonia alloy ACB C18150 is an age-hardenable zirconium chromium copper alloy with high electrical conductivity, hardness, and ductility; moderate strength; and excellent resistance to softening at elevated temperatures. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2018) 67 (11): cu-881.
Published: 01 November 2018
... workability thermal properties UNS C42500 Alloy CuSn3Zn9 is a bronze alloy. Chemical Composition, wt.% (Nominal) Tin 1.5 3.5 Zinc 7.5 10.0 Phosphorus 0.2 max Copper bal Physical Properties Electrical Conductivity. Depending on temper. IACS: International Annealed Copper Standard Density, 20 °C (68 °F...
Journal Articles
Alloy Digest (2018) 67 (12): cu-882.
Published: 01 December 2018
... International®. All rights reserved. KEMPER CuSn6Zn6 (Copper Bronze Alloy) Filing Code: Cu-882 Copper :: December 2018 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.4634 :: www.asminternational.org :: MemberServiceCenter@asminternational.org Published by ASM International® :: Data shown are...
Journal Articles
Alloy Digest (2004) 53 (8): Cu-721.
Published: 01 August 2004
..., 30% of C36000 Fair Capacity for being mechanically Good polished Capacity for being electroplated Excellent Capacity for being hot-dip tinned Poor See also more detail under General Characteristics. WIELAND-S23 Filing Code: Cu-721 Copper August 2004 WIELAND-S23 (High-Zinc Copper Alloy) Wieland-S23...