1-20 of 252

Search Results for Copper alloy no. 360

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1974) 23 (3): Cu-276.
Published: 01 March 1974
... COPPER ALLOY No. 360 is a leaded brass suitable for high-speed screw-machine work. It has many uses such as hardware, gears and pinions. Its trade names include free-turning brass, free-cutting yellow brass and high-leaded brass. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1982) 31 (11): Cu-447.
Published: 01 November 1982
... ANACONDA Alloy 360 is a leaded brass and is the alloy most often used for high-speed machining operations; it fills most of the needs for such purposes. Alloy 360 is the standard free-cutting brass and its machinability has become the standard by which all other copper-base alloys are rated...
Journal Articles
Alloy Digest (1999) 48 (1): Cu-627.
Published: 01 January 1999
... conductivity hardness joinability Olin C197 physical properties tensile properties thermal conductivity wear resistance workability OLIN C197 (Higher Conductivity Copper) Olin C197 is a second-generation high performance alloy developed by Olin Brass. It has a strength and bend formability similar...
Journal Articles
Alloy Digest (1988) 37 (8): Ni-360.
Published: 01 August 1988
... JESSOP JS Alloy 400 is a nickel-copper alloy with an excellent combination of high strength, ductility and corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (1990) 39 (10): Al-308.
Published: 01 October 1990
... Aluminum Alloy 360 is a hypoeutectoid aluminum silicon die cast alloy with restricted copper content. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue. It also includes information on high temperature...
Journal Articles
Alloy Digest (1978) 27 (9): Cu-360.
Published: 01 September 1978
... fatigue properties flexible hose fracture toughness hardness heat treatability high-temperature alloys joinability low-temperature alloys machinability OLIN ALLOY 194 physical properties tensile properties workability UNS C19400 OLIN ALLOY 194 Filing Code: cu-360 Copper Alloy SEPTEMBER...
Journal Articles
Alloy Digest (1992) 41 (10): Ni-413.
Published: 01 October 1992
... are achieved with a pro- prietary heat treatment performed by Brush Wellman. With mill hardened material, heat treatment and associ- ated cleaning steps are unnecessary and shrinkage is eliminated. Removing Copper Plating: Alloy 360 purchased with a copper electroplated surface should be pickled to remove...
Journal Articles
Alloy Digest (1994) 43 (10): Cu-552.
Published: 01 October 1994
... Reduction during rolling, % Figure 1 -Tensile strength versus reduction during rolling for zirconium-copper (Cl 5100) compared to other copper alloys with low alloying Figure 3 -Softening resistance of lead frame materials at an intermediate temperature limit, 660°F (360 co-562-a ...
Journal Articles
Alloy Digest (1961) 10 (5): Al-103.
Published: 01 May 1961
... is a purer form of Composition: 360 Alloy A360 Alloy Silicon 9.0-10-o 9.0-10.0 Magnesium 0.4-0.6 0.4-0.6 Iron 2.0 max. 1.3 max. Copper 0.6 max. 0.6 max. Manganese 0.35 max. 0.35 max. Zinc 0.5 max. 0.5 max. Nickel 0.5 max. 0.5 max. Tin 0.15 max. 0.15 max. Other impurities 0.2 max. 0.2 max. Aluminum Remainder...
Journal Articles
Alloy Digest (2015) 64 (5): Cu-837.
Published: 01 May 2015
... Wieland-K42 is a copper alloy with a small amount of zinc for strength without removing its good copper physical properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information...
Journal Articles
Alloy Digest (1985) 34 (11): Ni-326.
Published: 01 November 1985
.... Strip that had been copper plated for increased tool life should bestripped prior to aging. Fixturing may be needed when dimensional accuracy must be closely controlled. .Alloy 360shrinksapproximatelyO.Z%in length. DOI: 10.31399/asm.ad.ni0326 Copyright © ASM International® 1996 Table 2 - RELATIVE...
Journal Articles
Alloy Digest (2020) 69 (1): Cu-903.
Published: 01 January 2020
... Olin Brass Alloy C10200 is an oxygen-free, high-conductivity copper. It is ideal for applications where extremely high electrical conductivity and resistance to hydrogen embrittlement are vital. Where glass-to-metal seals are required this material also provides the added advantage of developing...
Journal Articles
Alloy Digest (2005) 54 (1): Cu-728.
Published: 01 January 2005
... 2005 2005 ASM International bend strength cables chemical composition corrosion-resistant alloys elasticity electrical conductivity electrolytic tough pitch copper heat treatability joinability physical properties thermal conductivity WIELAND-K32 UNS C11000 Chemical Composition...
Journal Articles
Alloy Digest (2005) 54 (2): Cu-730.
Published: 01 February 2005
... specific conditions of service, copper is generally less subject to corrosion than other engineering metals. Copper often is used where resistance to corrosion is of prime importance. Sometimes, it is better to use a copper alloy rather than an unal- loyed copper. In general, copper resists nonoxidizing...
Journal Articles
Alloy Digest (1963) 12 (9): SA-153.
Published: 01 September 1963
... entering the welded joints. Pre- heats are not normally needed. It is recommended to use low hydrogen AWS spec. E-100Xx, E-110Xx and E-120Xx electrodes. Corrosion Resistance: Jalloy-AR steels are produced with the addition of copper and other alloys to enhance atmospheric corrosion resistance...
Journal Articles
Alloy Digest (2018) 67 (9): Cu-879.
Published: 01 September 2018
... Alloy Cu-ETP (UNS C11000) is a high conductivity pure copper alloy. The alloy is characterized by good electrical and thermal conductivity, and very good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, and bend strength. It also...
Journal Articles
Alloy Digest (2015) 64 (12): Cu-846.
Published: 01 December 2015
... Wieland-K15 is a deoxidized copper with low residual phosphorus. The alloy has good cold working properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2023) 72 (2): Cu-938.
Published: 01 February 2023
... Aurubis CuZn0.5 is a copper alloy deoxidized by the addition of zinc. It has good electrical conductivity (≥ 82% IACS), and higher strength as compared to pure copper. This alloy has very good welding and soldering properties because it is largely insensitive to hydrogen embrittlement...
Journal Articles
Alloy Digest (2015) 64 (11): Cu-843.
Published: 01 November 2015
... AM388 is a copper-base spinodal alloy with high strength combined with formability. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on forming and heat treating. Filing Code: Cu-843. Producer...
Journal Articles
Alloy Digest (2017) 66 (1): Cu-856.
Published: 01 January 2017
... Alloy KHP 102 (UNS C19010) is a high performance copper alloy with additions for strength while maintaining high conductivity. KHP 102 belongs to the group of CuNiSi alloys and is particularly suitable for use in electrical and electronic products. This datasheet provides information...