1-20 of 496 Search Results for

Copper alloy no. 350

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1974) 23 (4): Cu-277.
Published: 01 April 1974
... COPPER ALLOY No. 350 is a medium-leaded brass containing 0.8-1.4 lead. Its machinability is 70% of that of free-cutting brass. It is suitable for use in high-speed screw machine work and has many uses such as lock parts, templates, nuts and gears. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1980) 29 (12): Cu-407.
Published: 01 December 1980
... SOMERS LTA Copper is a wrought copper foil that can be annealed at 350 F in 15 minutes to the full-soft condition; its use simplifies the manufacture of printed circuits (LTA = Low-Temperature Annealable). LTA Copper is especially useful for foil weights up to and including one ounce per square...
Journal Articles
Alloy Digest (2020) 69 (9): Cu-912.
Published: 01 September 2020
... Schmelzmetall Hovadur CCZ is a heat-treatable, copper-chromium-zirconium alloy. In the solution heat-treated and artificially aged condition, this alloy exhibits high thermal and electrical conductivity along with high strength and a high softening temperature. Hovadur CCZ evolved from CuCr1...
Journal Articles
Alloy Digest (1986) 35 (1): Cu-505.
Published: 01 January 1986
... BRUSHFORM 290 is a specially processed, mill-hardened beryllium copper alloy having improved formability while maintaining the strength of other mill-hardened copper beryllium alloys. It was developed for current carrying springs requiring greater formability. It can be used in a number...
Journal Articles
Alloy Digest (2017) 66 (8): Cu-863.
Published: 01 August 2017
... Alloy KHP 151 (UNS C15100) is a high performance copper alloy with very high conductivity. Typical uses include lead frames for high-power electronic circuits, connectors, and switchblade jaws; and applications requiring high conductivity, moderate strength, good bend formability and good stress...
Journal Articles
Alloy Digest (2018) 67 (8): Cu-878.
Published: 01 August 2018
... Wieland K60 is an age hardenable copper alloy combining good electrical and thermal conductivity with high strength. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion and wear resistance as well...
Journal Articles
Alloy Digest (1970) 19 (12): CS-38.
Published: 01 December 1970
...-hydrogen electrodes and in removing moisture from plate surfaces prior to welding. Corrosion Resistance: LUKENS AR-350 has atmospheric corrosion resistance at least twice that of carbon steel to which no copper has been added. Specification Equivalent: USS AR-350. General Characteristics: LUKENS AR-350...
Journal Articles
Alloy Digest (1993) 42 (10): Cu-589.
Published: 01 October 1993
... Amperes* Metal-arc .035 20-26 100-200 (deep)-Positive .045 22-28 loo-250 l/l 6 29-32 25040 3/32 32-34 350-500 *Use low side of range for iron- or nickel-base alloys; middle of range for bronze alloys: high side for copper. ...
Journal Articles
Alloy Digest (1993) 42 (9): Cu-587.
Published: 01 September 1993
... Alloy Cu-587 - DIGEST- SEPTEMBER 1993 DATA ON WORLD WIDE METALS AND ALLOYS oc4pyrigf 19% Alby Digest, Inc. Att rights -. PuMshedl~y: Alloy Digest. Inc. I201-677-9161 Data shown am tyrid, not to be used /or 27 Canfield SIreel. Orange. N.J. 0706O I U.S.A. spsdkatbfl m ma/ dasign. COPPER-TRODE@ (Deoxidized...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-616.
Published: 01 October 1999
... WRM Alloy C15500 is a copper alloy with one of the best combinations of electrical, mechanical, and relaxation properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, machining...
Journal Articles
Alloy Digest (2002) 51 (8): Cu-687.
Published: 01 August 2002
... CN8) (Hardenable Copper Alloy) Swissmetal alloy SM275H is a hardenable Cu-Ni-Sn alloy with good workability and corrosion resistance. It is often used in the automotive industry for springs, contacts, and clips. Swissmetal is a registered trademark of The Swissmetal Group. Table 1 Mechanical...
Journal Articles
Alloy Digest (2023) 72 (10): Cu-942.
Published: 01 October 2023
... Aurubis CuFe0.1P is a low-alloyed, age hardened copper alloy. It combines very high electrical conductivity (≥ 84% IACS) and thermal conductivity with relatively high strength. The alloy has improved temperature resistance as well as good relaxation properties and is suited for welding...
Journal Articles
Alloy Digest (1987) 36 (1): Cu-520.
Published: 01 January 1987
... Elongation (2 in 9&c Hardness, Rockwell F 0.010-0.020 3700040000 9000- 12000 35-37 45-63 l *. lg 20-b > 1 mmmm~mIImmmmmmmmmmmm tI,mmmmCml1m0mm_m_m( mm~~ I C.R. 1 10 166 Log Exposure Time, Minutes Fig. 1 - Softening of ZHC COPPER (Cl51) at 350°C compared with other leadframe alloys. C.R.=Cold rolled...
Journal Articles
Alloy Digest (2001) 50 (6): Cu-667.
Published: 01 June 2001
... Wieland-K81 is a copper-tin alloy with strength and cold working characteristics that are useful in making lead-frames. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information...
Journal Articles
Alloy Digest (1977) 26 (11): Cu-344.
Published: 01 November 1977
... Copper Alloy No. 865 is a copper-zinc-aluminum-iron-manganese alloy that is classified as high-strength yellow brass. It has a tensile strength about 20,000 psi greater than that of the corresponding copper-zinc (yellow brass) alloy; however, it is around the low-strength end of the manganese...
Journal Articles
Alloy Digest (1979) 28 (1): Cu-365.
Published: 01 January 1979
... Copper Alloy No. 862 is a copper-zinc-aluminum-manganese-iron alloy; aluminum is the principal strengthening element. It is classified as a high-strength yellow brass; its typical tensile strength is 95,000 psi. It has an excellent combination of strength and ductility along with good resistance...
Journal Articles
Alloy Digest (2021) 70 (2): Al-473.
Published: 01 February 2021
... Properties 8.0 10.0 Element 0.20 See Tables 1 and 2. Silicon 1.3 2.1 Iron 0.25 0.45 Alloy Quality Index Copper 0.12 Magnesium 0.05 The addition of copper in conventional 3xx.x casting alloys Titanium 0.15 causes considerable loss of ductility because copper- and Others, each bal magnesium-containing...
Journal Articles
Alloy Digest (1969) 18 (7): W-13.
Published: 01 July 1969
... shapes by powder metallurgy and finished as necessary by machining or grinding. Joining: This alloy may be joined to itself and to other materials by copper brazing, silver soldering, soft soldering, and welding, although mechanical joining is preferred. Sinter brazing is also used to join the alloy...
Journal Articles
Alloy Digest (1963) 12 (4): Cu-127.
Published: 01 April 1963
... COPPER Alloy No. 385 is a free-machining leaded brass recommended for hardware and architectural trim. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-620.
Published: 01 October 1999
... WRM Alloy 194-9 is a modified C19400 with mechanical properties far exceeding the conventional composition (see COPPER ALLOY No. 194, Alloy Digest Cu-233, May 1971). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...