Alloy Digest (1975) 24 (3): Cu-294.
Published: 01 March 1975
... Copper Alloy No. 330 is a brass containing nominally 0.5% lead. It has good machinability, excellent cold-working properties, and a wide range of uses including general purposes, industrial applications, munitions and plumbing. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1981) 30 (1): Cu-409.
Published: 01 January 1981
... physical properties plumbing goods power cylinders pumps tensile properties workability wrought brass UNS C33000 ANACONDA Alloy 330 Filing Code: cu409 copper Alloy JANUARY 19Bl - DATA ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980. Engineering Publications, Inc. WI rights reserved. ISSN : 002-6...
Journal Articles
Alloy Digest (1992) 41 (11): SS-537.
Published: 01 November 1992
... temperature strength combined with resistance to oxidation and carburization. The alloy is popular in the heat treating industry. Composition, Wt. %: Element Min Carbon Manganese Silicon 0.75 Phosphorus Sulfur Chromium 17.00 Nickel 34.00 Copper Lead Tin Iron* Remainder 0.10 2.00 1.50 0.03 0.03 20.00 37.00...
Journal Articles
Alloy Digest (2006) 55 (9): Cu-746.
Published: 01 September 2006
... Hidurel 6 is a copper alloy with some chromium. It has high strength with high conductivity. The alloy has superior conductivity to Hidurel 5 (Alloy Digest Cu-607, July 1996) and is used for electrical applications where strength and brazing ability are major requirements. This datasheet provides...
Journal Articles
Alloy Digest (2006) 55 (10): Cu-747.
Published: 01 October 2006
... Hidurel 640 is a copper alloy with similar properties to Hidurel 6 (see Alloy Digest Cu-746, September 2006) with superior mechanical properties at high temperature. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear...
Journal Articles
Alloy Digest (1987) 36 (7): Cu-526.
Published: 01 July 1987
... Copper Alloy No. C44300 is a copper-zinc-tin alloy inhibited by arsenic; it is commonly known as inhibited admiralty metal or admiralty brass. It has a good combination of strength and ductility and good resistance to general corrosion. The small addition of arsenic (nominally 0.06%) is made...
Journal Articles
Alloy Digest (2014) 63 (7): Cu-833.
Published: 01 July 2014
... BrushForm 96 strip is a high-performance, heat treatable spinodal copper-nickel-tin alloy designed to provide optimal formability and strength characteristics in conductive spring applications. It is available in both pre-heat treated (mill hardened) and heat treatable (age hardenable) forms...
Journal Articles
Alloy Digest (2009) 58 (9): Cu-774.
Published: 01 September 2009
... on forming, heat treating, machining, and joining. Filing Code: CU-774. Producer or source: Ansonia Copper & Brass Inc. Producer or Source: Ansonia Copper & Brass Inc. Copyright © ASM International® 2009 2009 ASM International ANSONIA ALLOY C24000 chemical composition elasticity...
Journal Articles
Alloy Digest (1980) 29 (2): Ag-8.
Published: 01 February 1980
... similar to that of silver. It tarnishes on exposure to sulfur and sulfur compounds at about the same rate as silver. Because it contains no copper, its resistance to salt corrosion is excellent. Production: Consil 900 is preoxidized silver-cadmium oxide. Cast and wrought alloys of silver and cadmium...
Journal Articles
Alloy Digest (1994) 43 (11): Cu-599.
Published: 01 November 1994
... COPPER ALLOY NOS. C44400 and C44500 are copper-zinc-tin alloys inhibited by antimony and phosphorus, respectively. They are commonly known as inhibited admiralty metal or admiralty brass. They have a good combination of strength and ductility and good resistance to general corrosion. The small...
Journal Articles
Alloy Digest (1993) 42 (12): Cu-594.
Published: 01 December 1993
... COPPER ALLOY NOS. C14300 AND C14310 are deoxidized coppers with a small percentage of Cd to resist thermal softening. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, machining...
Journal Articles
Alloy Digest (2009) 58 (10): Cu-775.
Published: 01 October 2009
..., and shear strength as well as fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: CU-775. Producer or source: Ansonia Copper & Brass Inc. Producer or Source: Ansonia Copper & Brass Inc. Copyright © ASM International® 2009 2009 ASM...
Journal Articles
Alloy Digest (1993) 42 (5): Cu-583.
Published: 01 May 1993
... Copper No. C15710 is a dispersion strengthened alloy with alumina. The strength is higher than copper while maintaining good electrical properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2001) 50 (6): Cu-668.
Published: 01 June 2001
... in., % Hardness, HV Annealed 240 34.80 180 26.10 32 80 1 2 hard (30%) 290 42.05 240 34.80 15 100 Hard (75%) 360 52.20 330 47.85 8 115 0.020 0.315 in. dimension DOI: 10.31399/asm.ad.cu0668 General Characteristics: SM453C is a free-machining copper alloy with high electrical conductivity. Product Forms Available...
Journal Articles
Alloy Digest (2008) 57 (5): Mn-4.
Published: 01 May 2008
... between 1.0 and 70 mm (0.039 and 2.76 in.) and thicknesses between 0.10 and 2.5 mm (0.0039 and 0.097 in Alloy Designation Portion of thickness, % High-expansive component 72-18-10 411 43.5 Low-expansive component Invar 450 38.7 Intermediate component Copper 470 17.8 DATA ON WORLDWIDE METALS AND ALLOYS...
Journal Articles
Alloy Digest (1986) 35 (11): Ni-342.
Published: 01 November 1986
... Digest. inc. 27 Canfield Street Orange. New Jersey 07050 (201) 761-1090 Composition: Nickel* 67.0 min. Carbon 0. IO max. Manganese 2.5-3. s Iron 3.0 max. Sulfur 0.015 max. Silicon 0.50 max. Copper 0.50 max. Chromium 18.0-22.0 Titanium 0.75 max. Columbium** 2.0-3.0 Phosphorus 0.03 max. Others 0.50 max...
Journal Articles
Alloy Digest (2006) 55 (6): Cu-744.
Published: 01 June 2006
... The Hiduron series of alloys are medium-strength copper-nickel alloys that offer excellent corrosion resistance and good impingement erosion resistance. Hiduron 107 is a medium-strength corrosion-resistant copper-nickel alloy that is often used in seawater applications. This datasheet provides...
Journal Articles
Alloy Digest (2007) 56 (6): Cu-748.
Published: 01 June 2007
... tensile properties workability high-temperature alloys thermal properties UNS C19720 Chemical Composition, wt Iron 0.05 0.50 Magnesium 0.06 0.20 Phosphorus 0.05 0.15 Tin 0.20 max Zinc 0.20 max Nickel 0.10 max Lead 0.05 max Manganese 0.05 max Copper plus named elements 99.5 min Copper bal Physical...
Journal Articles
Alloy Digest (2018) 67 (11): cu-881.
Published: 01 November 2018
... workability thermal properties UNS C42500 Alloy CuSn3Zn9 is a bronze alloy. Chemical Composition, wt.% (Nominal) Tin 1.5 3.5 Zinc 7.5 10.0 Phosphorus 0.2 max Copper bal Physical Properties Electrical Conductivity. Depending on temper. IACS: International Annealed Copper Standard Density, 20 °C (68 °F...
Journal Articles
Alloy Digest (1993) 42 (9): Cu-587.
Published: 01 September 1993
... Gas Tungsten-arc Filler Diameter Amperes* (dcen) Amperes* (achf) l/16 70-120 70-150 3/32 120-160 140-230 l/8 170-230 225-320 5i32 220-280 175-300 3116 280-330 200-320 *Use low side of range for iron- or nickel-base alloys; middle of range for bronze alloys; high side for copper. DOI: 10.31399...