Skip Nav Destination
Close Modal
Search Results for
Copper alloy no. 280
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 176 Search Results for
Copper alloy no. 280
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1974) 23 (8): Cu-282.
Published: 01 August 1974
... Copper Alloy No. 280 is a 60-40 copper-zinc alloy having good strength but low ductility. It has good hot working properties and good general resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear...
Abstract
View article
PDF
Copper Alloy No. 280 is a 60-40 copper-zinc alloy having good strength but low ductility. It has good hot working properties and good general resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-282. Producer or source: Copper and copper alloy mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (6): Cu-418.
Published: 01 June 1981
... ANACONDA Alloy 280 is nominally a 60% copper-40% zinc alloy with good strength but low ductility. It has excellent hot-working characteristics but its capacity for being cold-worked is only fair. Alloy 280 has a pleasing, reddish-yellow color much like that of extruded architectural bronze. Among...
Abstract
View article
PDF
ANACONDA Alloy 280 is nominally a 60% copper-40% zinc alloy with good strength but low ductility. It has excellent hot-working characteristics but its capacity for being cold-worked is only fair. Alloy 280 has a pleasing, reddish-yellow color much like that of extruded architectural bronze. Among its many uses are architectural applications, trim, hot forgings, condenser plates and heat exchanger tubes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-418. Producer or source: Anaconda American Brass Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1974) 23 (6): Cu-280.
Published: 01 June 1974
... COPPER Alloy No. 425 is a copper-zinc-tin alloy suitable for electrical switches and springs, fuse and pen clips, and weather stripping. It can be cold worked readily by convectional processes. This datasheet provides information on composition, physical properties, hardness, elasticity...
Abstract
View article
PDF
COPPER Alloy No. 425 is a copper-zinc-tin alloy suitable for electrical switches and springs, fuse and pen clips, and weather stripping. It can be cold worked readily by convectional processes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-280. Producer or source: Brass mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (7): Cu-619.
Published: 01 July 1998
... WRM alloy 4252 is a modified copper-zinc-tin alloy similar to C42500 (see Alloy Digest Cu-280, June 1974), with improved conductivity, strength, and forming properties. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: CU-619. Producer...
Abstract
View article
PDF
WRM alloy 4252 is a modified copper-zinc-tin alloy similar to C42500 (see Alloy Digest Cu-280, June 1974), with improved conductivity, strength, and forming properties. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: CU-619. Producer or source: Waterbury Rolling Mills Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (10): Ni-280.
Published: 01 October 1982
... NICROFER 3620 Cb is a nickel-chromium-copper-molybdenum alloy that is stabilized (against intergranular corrosion) by columbian. It is resistant to corrosion in a wide variety of oxidizing and reducing media. This alloy is used extensively in various areas of the chemical industry. This datasheet...
Abstract
View article
PDF
NICROFER 3620 Cb is a nickel-chromium-copper-molybdenum alloy that is stabilized (against intergranular corrosion) by columbian. It is resistant to corrosion in a wide variety of oxidizing and reducing media. This alloy is used extensively in various areas of the chemical industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-280. Producer or source: Vereingte Deutsche Metallwerke AG.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (9): Cu-587.
Published: 01 September 1993
... Gas Tungsten-arc Filler Diameter Amperes* (dcen) Amperes* (achf) l/16 70-120 70-150 3/32 120-160 140-230 l/8 170-230 225-320 5i32 220-280 175-300 3116 280-330 200-320 *Use low side of range for iron- or nickel-base alloys; middle of range for bronze alloys; high side for copper. DOI: 10.31399...
Abstract
View article
PDF
COPPER-TRODE provides quality deposits with high electrical conductivity. Virgin copper is used. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-587. Producer or source: Ampco Metal Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (11): Cu-935.
Published: 01 November 2022
... Austral Wright Copper Alloy 220 (UNS C22000), also known as 90/10 gilding metal, is a wrought copper-zinc alloy. It combines a rich golden color with the best combination of strength, ductility, and corrosion resistance of the plain copper-zinc alloys. It weathers to a rich bronze color and can...
Abstract
View article
PDF
Austral Wright Copper Alloy 220 (UNS C22000), also known as 90/10 gilding metal, is a wrought copper-zinc alloy. It combines a rich golden color with the best combination of strength, ductility, and corrosion resistance of the plain copper-zinc alloys. It weathers to a rich bronze color and can be supplied in pre-patinated colors ranging from deep brown to green. Austral Wright Copper Alloy 220 has a lower rate of work hardening than the copper-zinc alloys with higher zinc content, such as alloys 260 and 272. This is an advantage in multistage pressing applications without interstage annealing. It has excellent deep drawing characteristics and resistance to pitting corrosion when exposed to severe weather and water environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Cu-935. Producer or source: Austral Wright Metals.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (9): Cu-787.
Published: 01 September 2010
.... AMPCOLOY® 88 (High-Performance Copper Alloy) AMPCOLOY® 88 Chemical Composition, wt (Nominal) Cobalt + Nickel 3 Beryllium 0.5 Others 0.5 max Copper bal Physical Properties: Density, g/cm3 (lb/in.3) 8.75 (0.315) Coefficient of thermal expansion, 10 6 /K (10 6/ºF) 17 (9.44) Electrical conductivity, 106S/m...
Abstract
View article
PDF
Ampcoloy 88 was developed for plastic tooling and has a hardness greater than 260 HB, a high thermal conductivity, with good machinability and polishability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: CU-787. Producer or source: AMPCO Engineered Alloys.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2014) 63 (7): Cu-833.
Published: 01 July 2014
... BrushForm 96 strip is a high-performance, heat treatable spinodal copper-nickel-tin alloy designed to provide optimal formability and strength characteristics in conductive spring applications. It is available in both pre-heat treated (mill hardened) and heat treatable (age hardenable) forms...
Abstract
View article
PDF
BrushForm 96 strip is a high-performance, heat treatable spinodal copper-nickel-tin alloy designed to provide optimal formability and strength characteristics in conductive spring applications. It is available in both pre-heat treated (mill hardened) and heat treatable (age hardenable) forms. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. and bend strength. It also includes information on forming. Filing Code: Cu-833. Producer or source: Materion Brush Performance Alloys.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (12): Pd-2.
Published: 01 December 2016
... Paliney H3C is a palladium, copper and silver based alloy designed for applications such as semiconductor test probes where extreme hardness and higher levels of electrical conductivity are required. This datasheet provides information on physical properties, hardness, elasticity, and tensile...
Abstract
View article
PDF
Paliney H3C is a palladium, copper and silver based alloy designed for applications such as semiconductor test probes where extreme hardness and higher levels of electrical conductivity are required. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: Pd-2. Producer or source: Deringer Ney.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (12): Al-383.
Published: 01 December 2002
.... Specification Equivalents: ANSI/AWS A5.10 (ER and R) ANSI/AWS A5.8 AMS 4184 Brazing alloy BAlSi3 UNS A94145 General Characteristics: Alloy 4145 was originally developed as a brazing alloy because of its low melting temperature and high fluidity. The principal alloy- ing elements are silicon and copper...
Abstract
View article
PDF
AlcoTec weld filler wire 4145 is a general-purpose high-silicon-containing wire for both welding and brazing. The alloy is often used instead of 2319 for welding higher-strength alloys because of its low melting temperature and high fluidity. This datasheet provides information on composition and physical properties. It also includes information on joining. Filing Code: AL-383. Producer or source: AlcoTec Wire Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (7): Al-466.
Published: 01 July 2020
... Alcoa 351 SupraCast is a heat-treatable aluminum-silicon-copper alloy that also contains small amounts of magnesium, manganese, vanadium, and zirconium. It is designed for components exposed to elevated temperatures in high performance engines. This datasheet provides information on composition...
Abstract
View article
PDF
Alcoa 351 SupraCast is a heat-treatable aluminum-silicon-copper alloy that also contains small amounts of magnesium, manganese, vanadium, and zirconium. It is designed for components exposed to elevated temperatures in high performance engines. This datasheet provides information on composition, physical properties, and tensile properties as well as fatigue. It also includes information on heat treating, machining, and joining. Filing Code: Al-466. Producer or source: Alcoa Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (7): Al-379.
Published: 01 July 2002
... controls on the elements that make up aluminum alloys used to contain the chemicals. Alloy 5654 was originally developed in 1968 to pro- vide controlled low limits of manganese and copper. The result was a filler alloy that can be used to weld tanks for storage of hydrogen peroxide. Because this alloy...
Abstract
View article
PDF
AlcoTec Weld Filler Wire 5654 is a nonheatable wire with moderate high-strength capabilities. The principal alloying elements are magnesium, manganese, chromium, and titanium. This datasheet provides information on composition, physical properties, and shear strength. It also includes information on corrosion resistance as well as joining. Filing Code: AL-379. Producer or source: AlcoTec Wire Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (11): Al-382.
Published: 01 November 2002
... Alcotec weld filler wire 2319 is a heat treatable wire. The principal alloying elements are copper, manganese, vanadium, zirconium, and titanium. Weld filler wire 2319 was developed primarily for aircraft structural components to weld the high-strength age-hardenable wrought alloy 2219...
Abstract
View article
PDF
Alcotec weld filler wire 2319 is a heat treatable wire. The principal alloying elements are copper, manganese, vanadium, zirconium, and titanium. Weld filler wire 2319 was developed primarily for aircraft structural components to weld the high-strength age-hardenable wrought alloy 2219. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on joining. Filing Code: AL-382. Producer or source: AlcoTec Wire Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1969) 18 (8): Ni-146.
Published: 01 August 1969
... sulphuric acid. The alloy is capable of being age hardened. Composition: Physical Constants: Chromium 28.00 Specific gravity 8.57 Molybdenum 8.00 Copper 5.50 Silicon 3.50 Manganese 1 .oo Iron 1.50 Carbon 0.05 Nickel Remainder (Where added ductility or conversely higher hardness is required. the chemistry...
Abstract
View article
PDF
ILLIUM B was developed as a bearing alloy for maximum wear and galling resistance in high concentrations of hot sulfuric acid. The alloy is capable of being age hardened. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Ni-146. Producer or source: Stainless Foundry & Engineering Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2008) 57 (11): Cu-761.
Published: 01 November 2008
... strength, MPa (ksi) Elongation (2 in min, % Soft 350 (51) 550 (80) 45 ½ hard 550 (80) 700 (102) 32 Hard 800 (116) 920 (134) 5 Extra-spring 950 (138) 1035 (150) Fig. 1 Yield strength Fig. 2 Tensile strength DATA ON WORLDWIDE METALS AND ALLOYS Filing Code: Cu-761 Copper November 2008 Copyright © 2008, ASM...
Abstract
View article
PDF
Swissmetal B14 attains high strength by aging after cold working. It is used in springs. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CU-761. Producer or source: Avins Industrial Products.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (11): Cu-655.
Published: 01 November 2000
... bronze that produces a fine surface finish. Applications are in springs, demanding large elastic deformations. Swissmetal is a registered trademark of Swissmetal Boillat. Chemical Composition, wt Iron 0.02 max Lead 0.40 0.60 Tin 13.10 13.90 Copper bal Physical Properties: Density, kg/m3 (lb/in.3 ) 8691...
Abstract
View article
PDF
Swissmetal alloy SM802K is a free-machining bronze that produces a fine surface finish. Applications are in springs, demanding large elastic deformations. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-655. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2018) 67 (7): Cu-875.
Published: 01 July 2018
... Alloy CuSn8 (UNS C52100) is a high-performance copper alloy with 8% tin. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on wear resistance as well as forming and joining. Filing Code: Cu-875...
Abstract
View article
PDF
Alloy CuSn8 (UNS C52100) is a high-performance copper alloy with 8% tin. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on wear resistance as well as forming and joining. Filing Code: Cu-875. Producer or source: Gebr. Kemper GmbH + Company KG Metallwerke.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (12): Cu-695.
Published: 01 December 2002
... compressive strength hardness heat treatability joinability physical properties shear strength Swissmetal alloy SM931R tensile properties workability thermal properties Chemical Composition, wt Copper 59.0 61.0 Zinc bal Aluminum 0.3 0.7 Lead 0.5 max Tin 0.5 max Iron 0.3 max Nickel 0.3 max Total...
Abstract
View article
PDF
Swissmetal alloy SM931R is an alloy designed for hot working and contains a duplex alpha plus beta microstructure. The alloy has also been called DORECO. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and shear strength. It also includes information on forming, heat treating, and joining. Filing Code: CU-695. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (11): Cu-578.
Published: 01 November 1992
... BRUSH WELLMAN Alloy 174 is a beryllium copper alloy with cobalt designed to be a current-carrying component where high strength and relaxation resistance alloys are needed for body downsizing and miniaturization of microprocessors. This datasheet provides information on composition, physical...
Abstract
View article
PDF
BRUSH WELLMAN Alloy 174 is a beryllium copper alloy with cobalt designed to be a current-carrying component where high strength and relaxation resistance alloys are needed for body downsizing and miniaturization of microprocessors. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on forming and heat treating. Filing Code: Cu-578. Producer or source: Brush Wellman Inc.. See also Alloy Digest Cu-509, May 1986.