Skip Nav Destination
Close Modal
Search Results for
Copper alloy no. 165
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 222 Search Results for
Copper alloy no. 165
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (2): Cu-327.
Published: 01 February 1977
... Copper Alloy No. 165 is a copper-cadmium-tin alloy with low strength and high ductility in the annealed condition. In the hard-drawn condition, characterized by high strength and low ductility, it is used widely as an electrical conductor. This datasheet provides information on composition...
Abstract
View article
PDF
Copper Alloy No. 165 is a copper-cadmium-tin alloy with low strength and high ductility in the annealed condition. In the hard-drawn condition, characterized by high strength and low ductility, it is used widely as an electrical conductor. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-327. Producer or source: Copper and copper alloy mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (12): Cu-532.
Published: 01 December 1987
... BRUSH Alloy 165 has slightly less yield and fatigue strengths than the somewhat higher beryllium-content copper-beryllium alloy. It is cheaper and may be substituted when design requirements are less demanding. It is easily worked to provide complex shapes. This datasheet provides information...
Abstract
View article
PDF
BRUSH Alloy 165 has slightly less yield and fatigue strengths than the somewhat higher beryllium-content copper-beryllium alloy. It is cheaper and may be substituted when design requirements are less demanding. It is easily worked to provide complex shapes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Cu-532. Producer or source: Brush Wellman Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (10): Cu-423.
Published: 01 October 1981
... corrosion-resistant alloys durability elasticity electrical conductivity fatigue properties hardness heat treatability HITENSO 165 joinability machinability physical properties railroad switches tensile strength workability wrought copper alloys UNS C16500 HITEWSO 165 Filing Code: Cu423...
Abstract
View article
PDF
HITENSO 165 offers an excellent and difficult-to-acquire combination of high tensile strength and good electrical conductivity. The nominal composition of 98.58% copper with cadmium, tin and silver gives it high-strength and wear characteristics while retaining good conductivity. It is used as trolley wire because of its exceptional durability for curves and switches on electrified railroads carrying heavy traffic and for trackless trolleys where wear is high. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-423. Producer or source: Anaconda Industries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1963) 12 (4): Cu-20.
Published: 01 April 1963
... Berylco 165 is a lower cost version of the standard 1.9 percent beryllium copper alloy. It offers good formability in the unhardened condition with high final properties following precipitation hardening. It is also available in the mill hardened condition which, without heat treatment...
Abstract
View article
PDF
Berylco 165 is a lower cost version of the standard 1.9 percent beryllium copper alloy. It offers good formability in the unhardened condition with high final properties following precipitation hardening. It is also available in the mill hardened condition which, without heat treatment by the fabricator, reaches strengths and hardnesses appreciably higher than bronze. Through good formability, it offers cost-saving opportunities by eliminating hardening. It combines good ductility with high strength and hardness, good electrical and thermal conductivity, and excellent resistance to wear and fatigue. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Cu-20. Producer or source: Beryllium Corporation. Originally published November 1954, revised April 1963.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1966) 15 (6): Cu-165.
Published: 01 June 1966
... hardness heat treatability joinability machinability physical properties shear strength tensile properties thermal conductivity wear resistance workability Filing Code: Cu-165 I -. COPPER ALLOY No 172 Copper Alloy JUNE 1966 -DATA ON WORLD WIDE METALS AND ALLOYS Pvblisbed by COPPER ALLOY No. 172...
Abstract
View article
PDF
Copper Alloy No. 172 is a precipitation hardening beryllium-copper alloy having high elastic and endurance strength, good electrical and thermal conductivity, excellent resistance to wear, and high resistance to general corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-165. Producer or source: Copper and copper alloy mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1991) 40 (1): Al-311.
Published: 01 January 1991
... ALLOY 380 is an aluminum/silicon die casting alloy with controlled copper content (3-4%). This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue. It also includes information on high temperature performance...
Abstract
View article
PDF
ALLOY 380 is an aluminum/silicon die casting alloy with controlled copper content (3-4%). This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting and heat treating. Filing Code: Al-311. Producer or source: Aluminum Smelting and Refining Company Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2014) 63 (6): Cu-832.
Published: 01 June 2014
...-338-5151 MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Cu-832 Copper June 2014 BrushForm 158 is a spinodal alloy that develops exceptionally high elastic strength levels, dimensional stability, and relaxation resistance at high temperatures. BRUSHFORM®...
Abstract
View article
PDF
BrushForm 158 is a spinodal alloy that develops exceptionally high elastic strength levels, dimensional stability, and relaxation resistance at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. and bend strength. It also includes information on forming. Filing Code: Cu-832. Producer or source: Materion Brush Performance Alloys.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (9): Cu-588.
Published: 01 September 1993
... COPPER ALLOY NO. C72900 is a spinodal alloy that develops exceptionally high elastic strength levels; dimensional stability and relaxation resistance at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Abstract
View article
PDF
COPPER ALLOY NO. C72900 is a spinodal alloy that develops exceptionally high elastic strength levels; dimensional stability and relaxation resistance at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: CU-588. Producer or source: Copper and copper alloy mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (10): Ni-304.
Published: 01 October 1984
... NICLOY 400 is a nickel-copper, solid-solution alloy which is utilized in numerous applications because of its good mechanical strength and overall excellent resistance to corrosion. Among its many uses are pump parts, marine fixtures, oil production and refining equipment, heat exchangers...
Abstract
View article
PDF
NICLOY 400 is a nickel-copper, solid-solution alloy which is utilized in numerous applications because of its good mechanical strength and overall excellent resistance to corrosion. Among its many uses are pump parts, marine fixtures, oil production and refining equipment, heat exchangers and numerous machined parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-304. Producer or source: Babcock & Wilcox Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1976) 25 (5): Cu-312.
Published: 01 May 1976
..., hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-312. Producer or source: Copper and copper alloy mills. Producer or Source: Copper and copper alloy mills...
Abstract
View article
PDF
Copper No. 150 contains nominally 0.15% zirconium. It retains high conductivity with good hardness, strength and ductility at elevated temperatures. Applications include collector rings, bearings and current-carrying shafts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-312. Producer or source: Copper and copper alloy mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (11): Cu-853.
Published: 01 November 2016
... workability thermal properties UNS C14415 Kobelco Alloy KFC has very high conductivity for leadframe applications. Chemical Composition, wt (Typical analysis) Iron 0.1 Phosphorus 0.03 Copper bal Physical Properties: Specific gravity 8.9 Coefficient of thermal expansion, 20~300 °C (58~572 °F), 10 6/K (10...
Abstract
View article
PDF
Kobelco Alloy KFC has very high conductivity for leadframe applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. and bend strength. It also includes information on forming. Filing Code: Cu-853. Producer or source: Kobe Steel Ltd, Aluminum and Copper Business.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (4): Ni-312.
Published: 01 April 1985
... NICORROS 400 is a nickel-copper, solid-solution alloy having excellent corrosion resistance in a wide range of marine and chemical environments and good mechanical properties from sub-zero temperatures to about 900 F. Among its uses are pump parts, heat exchangers, petroleum production...
Abstract
View article
PDF
NICORROS 400 is a nickel-copper, solid-solution alloy having excellent corrosion resistance in a wide range of marine and chemical environments and good mechanical properties from sub-zero temperatures to about 900 F. Among its uses are pump parts, heat exchangers, petroleum production and refinery equipment and marine equipment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-312. Producer or source: Vereingte Deutsche Metallwerke AG.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (3): Al-486.
Published: 01 March 2022
... Rio Tinto 355.2 is a heat-treatable, aluminum-silicon-copper-magnesium casting alloy (3xx.x series). It is available in the form of ingots for remelting, for the production of sand and permanent mold castings. It is a high-strength alloy with many desirable characteristics. The presence of copper...
Abstract
View article
PDF
Rio Tinto 355.2 is a heat-treatable, aluminum-silicon-copper-magnesium casting alloy (3xx.x series). It is available in the form of ingots for remelting, for the production of sand and permanent mold castings. It is a high-strength alloy with many desirable characteristics. The presence of copper in alloy 355.0 increases strength but reduces corrosion resistance and ductility. This alloy is less ductile than 356.0. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-486. Producer or source: Rio Tinto.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (5): W-25.
Published: 01 May 2001
... ELKONITE 1W3, 3W3, 3W53, 5W3, 10W3, 10W53, 30W3, 40W3, 50W3,and 2050C are a series of tungsten-copper compositions with the tungsten content ranging from 50 to 90 wt.%. These alloys are normally made by the press-sinter-infiltrate (PSI) method. This datasheet provides information on composition...
Abstract
View article
PDF
ELKONITE 1W3, 3W3, 3W53, 5W3, 10W3, 10W53, 30W3, 40W3, 50W3,and 2050C are a series of tungsten-copper compositions with the tungsten content ranging from 50 to 90 wt.%. These alloys are normally made by the press-sinter-infiltrate (PSI) method. This datasheet provides information on composition, physical properties, microstructure, and bend strength. It also includes information on heat treating. Filing Code: W-25. Producer or source: CMW Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (4): Al-463.
Published: 01 April 2020
... Rio Tinto Alloy 242.2 is a heat-treatable, aluminum-copper-magnesium-nickel casting alloy. It is available in the form of ingots to be remelted for the manufacture of sand and permanent mold castings. Alloy 242.0 is used extensively for applications requiring high strength and hardness at elevated...
Abstract
View article
PDF
Rio Tinto Alloy 242.2 is a heat-treatable, aluminum-copper-magnesium-nickel casting alloy. It is available in the form of ingots to be remelted for the manufacture of sand and permanent mold castings. Alloy 242.0 is used extensively for applications requiring high strength and hardness at elevated temperatures. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as casting, machining, and joining. Filing Code: Al-463. Producer or source: Rio Tinto Limited.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2018) 67 (6): Cu-873.
Published: 01 June 2018
... Alloy CuSn6 (UNS C51900) is a high-performance copper alloy. Typical uses include components for the electronics industry such as connector springs, relays, leaf springs, and switches as well as machine parts. This datasheet provides information on composition, physical properties, hardness...
Abstract
View article
PDF
Alloy CuSn6 (UNS C51900) is a high-performance copper alloy. Typical uses include components for the electronics industry such as connector springs, relays, leaf springs, and switches as well as machine parts. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Cu-873. Producer or source: Gebr. Kemper GmbH + Company KG Metallwerke.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1958) 7 (2): Cu-59.
Published: 01 February 1958
... BERYLCO-10CR is a heat treatable, beryllium-copper casting alloy having high elastic and endurance strength, high ductility and impact strength, and high electrical and thermal conductivity. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Abstract
View article
PDF
BERYLCO-10CR is a heat treatable, beryllium-copper casting alloy having high elastic and endurance strength, high ductility and impact strength, and high electrical and thermal conductivity. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, heat treating, machining, joining, and surface treatment. Filing Code: Cu-59. Producer or source: Beryllium Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (8): Cu-621.
Published: 01 August 1998
... (19.0) 0.3 Processing: Most copper alloys achieve their properties through the addition of alloy- ing elements and cold rolling. Beryllium copper alloys achieve their properties through alloying elements, cold rolling, and a precipitation hardening heat treatment. Before rolling to final thickness...
Abstract
View article
PDF
Olin 172 (UNS C17200) has a relatively high beryllium content and the ability to reach tensile strengths near 1380 MPa (200 ksi) This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming and heat treating. Filing Code: CU-621. Producer or source: Olin Brass.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2018) 67 (8): Cu-877.
Published: 01 August 2018
... Alloy CuSn10 is a high-performance copper alloy. The alloy is characterized by good electrical and thermal conductivity and very good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength...
Abstract
View article
PDF
Alloy CuSn10 is a high-performance copper alloy. The alloy is characterized by good electrical and thermal conductivity and very good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on corrosion and wear resistance as well as forming and joining. Filing Code: Cu-877. Producer or source: Gebr. Kemper GmbH + Company KG Metallwerke.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1994) 43 (1): SS-560.
Published: 01 January 1994
... REMANIT 4539 is a low carbon corrosion resistant austenitic stainless steel with good levels of chromium, nickel, molybdenum, copper and nitrogen to show good resistance to reducing acids and chloride solutions. It was one of the early alloys used in flue gas desulfurization equipment...
Abstract
View article
PDF
REMANIT 4539 is a low carbon corrosion resistant austenitic stainless steel with good levels of chromium, nickel, molybdenum, copper and nitrogen to show good resistance to reducing acids and chloride solutions. It was one of the early alloys used in flue gas desulfurization equipment. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-560. Producer or source: Thyssen Stahl AG.