1-20 of 110 Search Results for

Copper alloy no. 101

Sort by
Journal Articles
Alloy Digest (1974) 23 (5): Cu-278.
Published: 01 May 1974
...: Copper and copper alloy mills Copyright © ASM International® 1996 1996 ASM International chemical composition Copper alloy no. 101 corrosion-resistant alloys elasticity electrical applications electronic applications fatigue properties fracture toughness hardness heat treatability...
Journal Articles
Alloy Digest (2003) 52 (8): Cu-706.
Published: 01 August 2003
... of strength, relaxation resistance, electrical conductivity, and very good formability. MILLER MHP 101 Filing Code: Cu-706 Copper August 2003 MILLER MHP 101 (Copper-Nickel, Tin-Bearing Alloy) Miller alloy MHP 101 has excellent cold working properties. The alloy is used for its combination of strength...
Journal Articles
Alloy Digest (1982) 31 (10): Cu-446.
Published: 01 October 1982
... Copper Alloy No. C84200 is a free-cutting copper-zinc-tin-lead alloy. It is characterized by good casting properties, moderate strength and ductility, good machinability and good resistance to corrosion. Formerly used named (not recommended) are 101, Leaded Semi-Red Brass and 80-5-2.5-12.5...
Journal Articles
Alloy Digest (1961) 10 (6): Cu-101.
Published: 01 June 1961
... tensile properties workability Filing Code: Cu-101 Copper Alloy JUNE 1961 - m --INK0 All1 Cl -DATA nhl WtWLCh WIDE UIVALC AUB AI 1 I w.. -.vm-w 1. .II mr .m-m- w mALOYS Pub&bed by CUNICO (Permanent Magnet Alloy) Enginea~ Alloys Dieat. Inc. Upper Montchir, Ner Jay CUNICO is a permanent magnet alloy...
Journal Articles
Alloy Digest (2000) 49 (2): Cu-647.
Published: 01 February 2000
... in Table 1. Filing Code: Cu-647 Copper February 2000 OLIN C654 Table 1 Mechanical Properties Tensile strength Yield strength Temper MPa ksi MPa ksi Elongation in 2 in., % Approximate hardness, HRB 1 4 hard 517 621 75 90 414 60 33 81 1 2 hard 593 696 86 101 545 79 23 92 3 4 hard 669 772 97 112 634 92 13 95...
Journal Articles
Alloy Digest (1976) 25 (4): Zn-27.
Published: 01 April 1976
... dried after cleaning. Cleaning after drawing is important because some lubricants can etch the zinc. Joinability: Microzinc alloy 100 ls readily soldered to itself and to other metals such as copper and brass alloys and mild steel. The sur- faces to be soldered should be clean and bright. All traces...
Journal Articles
Alloy Digest (2001) 50 (2): Cu-659.
Published: 01 February 2001
... composition corrosion-resistant alloys elasticity electrical conductivity hardness heat treatability joinability oxygen free copper physical properties tensile properties weldability WIELAND-K09 workability thermal properties UNS C10100 Wieland K09 is an oxygen-free copper with excellent...
Journal Articles
Alloy Digest (2016) 65 (10): Cu-852.
Published: 01 October 2016
... 0.0010 max Zinc bal This is a high conductivity copper which has in the annealed condition, a minimum conductivity of 58.0 × 106 S/m (100 %IACS) except for alloy C10200 which has a minimum conductivity of 58.5 × 106 S/m (101 %IACS). Cu determined by the difference between the impurity total and 100...
Journal Articles
Alloy Digest (2016) 65 (9): Cu-851.
Published: 01 September 2016
... Mueller Alloy C10100 is an oxygen-free copper used for automotive rectifiers and for electrical applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2020) 69 (4): Cu-907.
Published: 01 April 2020
... Cu-OFE chemical composition physical properties hardness elasticity tensile properties corrosion-resistant alloys workability machinability thermal properties UNS C10100 DOI: 10.31399/asm.ad.cu0907 AURUBIS Cu-OFE (Oxygen-Free, High Conductivity Copper) Filing Code: Cu-907 Copper :: April...
Journal Articles
Alloy Digest (2000) 49 (1): Cu-645.
Published: 01 January 2000
... Code: Cu-645 Copper January 2000 OLIN ALLOY C688 Table 1 Mechanical Properties Tensile strength Yield strength Elongation Approximate hardness, Temper MPa ksi MPa ksi in 2 in., % HRB Annealed 531 600 77 87 359 52 35 1/4 hard 600 696 87 101 524 76 19 90 1/2 hard 669 772 97 112 634 92 9 95 Hard 731 827...
Journal Articles
Alloy Digest (1961) 10 (3): Al-101.
Published: 01 March 1961
... or the babbitts and slight- ly better than the copper-lead and cadmium-base alloys. Noral 730 resists the type of chemical attack which takes place in engine oils. Forms Available: Permanent mold castings. Applications: Bearings and bushings. Solid bearings that do not need a backing material to give strength...
Journal Articles
Alloy Digest (1957) 6 (7): Cu-52.
Published: 01 July 1957
... NICKEL SILVER, 65-12 is a copper-nickel-zinc alloy having excellent workability, weldability and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1981) 30 (5): Cu-417.
Published: 01 May 1981
... ULTRONZE is a copper alloy also known as Olin Alloy 654. It bridges the gap between standard high-performance copper alloys and beryllium-copper alloys, thus enabling the design of parts with properties previously only attainable with more expensive materials. The alloy has superior stress...
Journal Articles
Alloy Digest (2019) 68 (6): Cu-890.
Published: 01 June 2019
... chemical composition corrosion-resistant alloys food processing applications medical equipment Olin Brass Alloy C77000 physical properties solderability spring applications stiffness switches wrought copper alloys thermal properties UNS C77000 Olin Brass Alloy C77000 is an excellent spring...
Journal Articles
Alloy Digest (1976) 25 (10): Ni-234.
Published: 01 October 1976
... is a low-carbon version of Nimag 100. *NIMAG is a registered Composition: trademark of Magnetics, Division Nominal Nickel Copper lron Manganese Carbon Silicon Sulfur 99.5 0.05 0.15 0.20 0.01 0.05 0.005 of Spang industries. Physical Constants: Density, lb/cu in. (At 70°F) Specific gravity Melting point...
Journal Articles
Alloy Digest (2019) 68 (9): Cu-896.
Published: 01 September 2019
... Olin Brass C76200 is a copper-nickel-zinc alloy developed to conserve nickel for national defense. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming. Filing Code: Cu-896. Producer or source: Olin Brass...
Journal Articles
Alloy Digest (2009) 58 (4): Cu-768.
Published: 01 April 2009
... treatability joinability machinability physical properties tensile properties Wieland-F12 workability thermal properties WIELAND-F12 (Resistance Alloy) Wieland-F12 is a resistance alloy with a low coefficient of electrical resistance. Chemical Composition, wt (Nominal) Manganese 12 Nickel 2 Copper...
Journal Articles
Alloy Digest (2019) 68 (10): Cu-897.
Published: 01 October 2019
... Olin Brass C75200 is a copper-nickel-zinc alloy with a silvery-white color making it look like silver or stainless steel. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming. Filing Code: Cu-897. Producer...
Journal Articles
Alloy Digest (1978) 27 (4): Cu-351.
Published: 01 April 1978
... CHASE 69000 is a high-strength copper alloy that exceeds the strength levels of phosphor bronzes and some beryllium copper alloys. It is an electronic grade of copper alloy with excellent hot and cold-working characteristics. It is available in strip form and can be joined by soldering, brazing...