Journal Articles
Publisher: Journals Gateway
Alloy Digest (1966) 15 (6): Cu-165.
Published: 01 June 1966
... Copper Alloy No. 172 is a precipitation hardening beryllium-copper alloy having high elastic and endurance strength, good electrical and thermal conductivity, excellent resistance to wear, and high resistance to general corrosion. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (3): Cu-631.
Published: 01 March 1999
... Alloy C7025 is a second generation, high performance alloy whose strength comes from an age hardening heat treatment similar to that used for the beryllium coppers. With stress relaxation resistance comparable to Be-Cu alloys C170/C172 (see Olin 170, Alloy Digest Cu-615, July 1998, and Olin 172...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (4): Cu-781.
Published: 01 April 2010
... Boehler Uddeholm alloy BeCu172 is a high-strength beryllium copper mold with high thermal conductivity. BeCu Alloy 172 can be supplied in the high-hard (HH) condition at approximately 40 HRC and in the low-hard (LH) condition at approximately 30 HRC. This alloy is used for applications...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1966) 15 (12): Cu-172.
Published: 01 December 1966
... tensile properties welding electrode tips workability CUBE-ALLOY Filing Code: Cu-172 Copper Alloy -DATA ON WORLD WIDE METALS AND ALLOYS DECEMBER 1966 CUBE-ALLOY PubWad by EngilKaingAIloysIlidat Upper Montdair, New ]a~ (Dispersion Hardened Copper) CUBE-ALLOY is a dispersion hardened copper recommended...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1976) 25 (3): Cu-310.
Published: 01 March 1976
... Equivalents: CDA Copper Alloy No. 172. RWMA Group A, Class 4. General Characteristics: Ampcoloy 83 is a precipitation-hardenable copper-beryllium alloy possessing a unique combination of electrical and mechan- ical properties. Through precipitation hardening it attains tensile strengths around 190,000 psi...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (8): Cu-621.
Published: 01 August 1998
...-lnn.ofg OLIN 172 (High Beryllium Copper) 01~ I72 has a relatively hrgh beryllium content and the ability to reach tensile strengths near 1380 MPa (200 ksi) Chemical Composition, wt Beryllium Nickel + cobalt Nickel + cobalt + roe Aluminum Silicon Copper 1.8~LXt0 0.20 min 0.6 max 0.20 max 0.20 max BalanCe...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (8): Cu-850.
Published: 01 August 2016
... Brush 1916 is a heat-treatable leaded copper-nickel alloy engineered for automatic screw machine applications. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: Cu-850...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (10): Cu-620.
Published: 01 October 1999
... WRM Alloy 194-9 is a modified C19400 with mechanical properties far exceeding the conventional composition (see COPPER ALLOY No. 194, Alloy Digest Cu-233, May 1971). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (8): Ni-319.
Published: 01 August 1985
... CARPENTER NICKEL-COPPER ALLOY 400 combines high strength (comparable to structural steel) and toughness over a wide temperature range. It can be strengthened by cold working. It has excellent resistance to many corrosive environments. This alloy has excellent mechanical properties at sub-zero...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (11): Ni-726.
Published: 01 November 2016
... or Source: MetalTek International Copyright © ASM International® 2016 2016 ASM International cast nickel alloys castability chemical composition heat treatability machinability MTEK M35-1 MTEK M35-2 physical properties tensile properties MTEK M35-1 and M35-2 are nickel copper casting...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (10): Cu-634.
Published: 01 October 1999
... WRM Alloy C19400 has one of the best combinations of electrical conductivity, mechanical strength, forming properties, and stress-relaxation resistance characteristics of high-performance copper alloys for electronic applications. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (11): Cb-25.
Published: 01 November 2000
... the same basic parameters as 300-series stainless steel. Contact the producer for information about spinning over welds. Machinability: The machinability of C103 and most niobium alloys may be compared generally to those of 316 stainless steel in reference to tool wear due to heat buildup and copper...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (10): Cu-590.
Published: 01 October 1993
... COPPER ALLOY NO. C11100 is commonly called anneal-resistant electrolytic copper. It offers resistance to softening at slightly elevated temperatures by the addition of cadmium, which raises the temperature at which recovery and recrystallization occur. Its fabricating characteristics are the same...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (10): Cu-897.
Published: 01 October 2019
... Olin Brass C75200 is a copper-nickel-zinc alloy with a silvery-white color making it look like silver or stainless steel. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming. Filing Code: Cu-897. Producer...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (6): Al-465.
Published: 01 June 2020
... Rio Tinto 304.1 is a heat-treatable, aluminum-silicon casting alloy that also contains small amounts of iron, manganese, magnesium, copper, and titanium. This alloy is available in the form of ingots for remelting, for the manufacture of die castings. Alloy 304.0 was developed as K-Alloy by Delphi...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (4): SS-1089.
Published: 01 April 2011
... Kubota Alloy CN-7M is an iron-chromium-nickel-molybdenum-copper alloy that has alloy additions to give the alloy resistance to reducing acids. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (7): Cu-800.
Published: 01 July 2011
..., and joining. Filing Code: Cu-800. Producer or source: Ansonia Copper & brass Inc.. Producer or Source: Ansonia Copper & Brass Inc. Copyright © ASM International® 2011 2011 ASM International ANSONIA ALLOY C 48500 chemical composition elasticity hardness heat treatability joinability...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (2): Al-473.
Published: 01 February 2021
... Properties 8.0 10.0 Element 0.20 See Tables 1 and 2. Silicon 1.3 2.1 Iron 0.25 0.45 Alloy Quality Index Copper 0.12 Magnesium 0.05 The addition of copper in conventional 3xx.x casting alloys Titanium 0.15 causes considerable loss of ductility because copper- and Others, each bal magnesium-containing...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (4): Cu-370.
Published: 01 April 1979
... on corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Cu-370. Producer or source: Copper alloy foundries. Producer or Source: Copper alloy foundries Copyright © ASM International® 1996 1996 ASM International cast copper alloys...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (6): Cu-525.
Published: 01 June 1987
...). psi,(MPa) As Cast Typrcal (sand) 72000 (496) 37000 (255) 20 B78 25000 ( 172) - Heat I rcated and Aged Minimum Typical Values Values 145000 ( I000) 150000 (1032) I35000 (932) I 40000 (966) 0 I c34 C38 90000 (620) 95000 (654) - 23000 ( 158) Heat Treatment: Machinability: Stress Relief: Heat Copper Alloy...