Alloy Digest (1980) 29 (6): Cu-397.
Published: 01 June 1980
... Copper Alloy No. C95800 is a copper-aluminum-nickel-iron-manganese alloy with high strength and hardness. It also is characterized by excellent resistance to corrosion and good resistance to fatigue and wear. It is suited for service up to 750 F. Typical uses comprise hubs and blades of ship...
Journal Articles
Alloy Digest (1978) 27 (4): Cu-352.
Published: 01 April 1978
... marine hardware nuts physical properties pickling equipment tensile properties wear resistance workability wrought bronze UNS C95800 C63200 Filing Code: cu-352 AMPCO 483 Copper Alloy APRIL 1978 - DATA ON WORLD WIDE METALS AND ALLOYS (Aluminum Bronze) AMPCO 483 is a copper-base alloy that can...