Alloy Digest (1980) 29 (5): Cu-394.
Published: 01 May 1980
... Copper Alloy No. 173 is a precipitation-hardenable beryllium-copper alloy with a lead addition of nominally 0.40% to give it fairly good machinability. By combining work hardening and precipitation hardening, tensile strengths in excess of 200,000 psi can be developed. This alloy is characterized...
Journal Articles
Alloy Digest (1967) 16 (1): Cu-173.
Published: 01 January 1967
... properties workability AlI Or DICIST INCRAMET 800 Filing Code: Cu-173 Copper Alloy JANUARY 1967 -DATA ON WORLD WIDE METALS AND ALLOYS Prblirbd by Eagioecriag Alloys Digest. Inc. INCRAMET 800 Upper Maatciair, New Jaw (Heat Resistant Copper Alloy) Incramet 800 is a copper-base alloy exhibiting an excellent...
Journal Articles
Alloy Digest (1999) 48 (7): Cu-637.
Published: 01 July 1999
... elements 99.7 min Physical Properties: Density, kg/m3 (lb/in.3) at 20 °C (68 °F) 8800 (0.318) Thermal conductivity, W/m · K (Btu/h ft °F) 173 (100) Electrical conductivity, %IACS 40 Modulus of elasticity, GPa (106 psi) 110 (16) See Table 1 for comparison with properties of other copper alloys. Heat...
Journal Articles
Alloy Digest (1974) 23 (8): Cu-283.
Published: 01 August 1974
... COPPER ALLOY NO. 953 is an age-hardenable alloy offering high strength and hardness, good resistance to fatigue and wear, and excellent corrosion resistance. It can be used at temperatures up to 750 F. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2017) 66 (4): Cu-859.
Published: 01 April 2017
... is a high performance copper alloy with high conductivity. Chemical Composition, wt (Nominal) Tin 0.10 0.15 Copper bal Physical Properties: Density, kg/m3 (lb/in.3) 8900 (0.32) Electrical conductivity, 106 S/m (%IACS) 46 (80) Thermal conductivity, W/m·K (Btu/(h·ft·°F)) 300 (173) Coefficient of thermal...
Journal Articles
Alloy Digest (2004) 53 (9): Cu-725.
Published: 01 September 2004
... 1.1 Iron 0.05 max Nickel 0.8 1.2 Phosphorus 0.03 0.07 Zinc 0.30 max Copper bal Copper plus named elements 99.7 min Physical Properties: Density, 20 °C (68 °F), kg/m3 8900 (0.322) (lb/in.3 ) Thermal conductivity, 20 °C 173 (100) (68 °F), W/m K (Btu/(ft h °F)) Resistivity, 20 °C (68 °F), µ m...
Journal Articles
Alloy Digest (1993) 42 (10): Cu-590.
Published: 01 October 1993
... COPPER ALLOY NO. C11100 is commonly called anneal-resistant electrolytic copper. It offers resistance to softening at slightly elevated temperatures by the addition of cadmium, which raises the temperature at which recovery and recrystallization occur. Its fabricating characteristics are the same...
Journal Articles
Alloy Digest (2019) 68 (10): Cu-897.
Published: 01 October 2019
... of thermal expansion, 20 300 °C (68 572 °F), 10 6/K (10 6/°F) 16.2 (9.0) Electrical resistivity, m ( circular-mil/ft) 0.287 (173) Copyright © 2019, ASM International®. All rights reserved. OLIN BRASS C75200 (Cu-Ni-Zn Alloy) Filing Code: Cu-897 Copper :: October 2019 Materials Park, Ohio 44073-0002...
Journal Articles
Alloy Digest (2019) 68 (2): Cu-884.
Published: 01 February 2019
... UNS CC22600 Olin Brass Alloy C22600 is a brass alloy with resistance to corrosion and has good electrical conductivity. Chemical Composition, wt.% (Nominal) Iron 0.05 max Copper 86.0 89.0 Copper plus named elements 99.8 Lead 0.05 max Zinc bal Physical Properties Electrical Conductivity. Depending...
Journal Articles
Alloy Digest (1982) 31 (4): Cu-435.
Published: 01 April 1982
... Copper Alloy No. C71300 contains nominally 75% copper and 25% nickel. It was developed for use as a U.S. coinage alloy. Normally it is not furnished for general consumer use; however, it can be purchased by anyone who has a valid use for it. It is characterized by a good combination of strength...
Journal Articles
Alloy Digest (2009) 58 (7): Cu-772.
Published: 01 July 2009
... includes information on forming, heat treating, machining, and joining. Filing Code: CU-772. Producer or source: Ansonia Copper & Brass Inc. Producer or Source: Ansonia Copper & Brass Inc. Copyright © ASM International® 2009 2009 ASM International ANSONIA ALLOY C22600 chemical...
Journal Articles
Alloy Digest (1996) 45 (6): SS-646.
Published: 01 June 1996
... 800 H and Uranus 800 HT. Uranus is a registered trademark of Creusot-Lotre lndustrie Chemical Composition, wt (Nominal value) Carbon Chromium Nickel Silicon Sulfur Copper Titanium Aluminum hOtI Phosphorus(a) 10.10 19.0-23.0 30.0-35.0 s1.0 so.005 10.75 0.15-0.60 0.15-0.60 Balance 4l.020 (a) Sulfur...
Journal Articles
Alloy Digest (2004) 53 (1): Fe-125.
Published: 01 January 2004
... expansion COPPER/INVAR/COPPER corrosion-resistant alloys elasticity hardness heat sinks heat treatability hybrid enclosures joinability metal cores physical properties power planes printed circuit boards tensile properties workability wrought metal products UNS K93600 Chemical Composition...
Journal Articles
Alloy Digest (1968) 17 (3): Al-173.
Published: 01 March 1968
... strength and formability with good finishing characteristics. Ir responds to an age-hardening heat treatment. Alloy 6563 is a modification of alloy 6063 with improved finishing characteristics and somewhat lower mechanical properties. Composition: Physical Constants: Silicon Magnesium Iron Copper Manganese...
Journal Articles
Alloy Digest (1969) 18 (11): Cu-208.
Published: 01 November 1969
... COPPER Alloy No. 752 is a deep drawing grade of nickel silver. It has high resistance to corrosion and tarnish. It is used primarily for drawn, spun and similar cold-worked parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1966) 15 (2): Cu-161.
Published: 01 February 1966
... EVERDUR-655 is a copper-silicon-manganese alloy having the desired combination of high strength, good workability, weldability and machinability along with high corrosion resistance. It is recommended for fasteners, springs pressure vessels and general hardware. This datasheet provides information...
Journal Articles
Alloy Digest (2007) 56 (1): SS-984.
Published: 01 January 2007
... tensile properties TRINAMET workability Chemical Composition, wt (Type Analysis) Carbon 0.30 max Phosphorus 0.040 max Silicon 1.00 max Molybdenum 1.00 3.00 Manganese 1.00 Sulfur 0.030 Chromium 12.00 14.00 Copper 2.00 3.00 Iron bal Physical Properties: Specific gravity 7.77 Density, kg/m3 (lb/in.3...
Journal Articles
Alloy Digest (1998) 47 (4): SS-711.
Published: 01 April 1998
... Coefficient of Thermal Expansion C&on Manganese Silicon Phosphorus Sulfur Chromium Nickel Copper Nitrogen Iron 0.15 max 6.50-9.00 l.OOmax 0.060 max 0.030 max 15.50-17.50 1.50-3.50 2.00-4.00 0.05-0.25 Balance listtrmpmam tzoen&aarlinsr-. . oc OF lo-c/K (10-W 2sKm n-212 17.1 950 25-150 n-302 173 9.61 254200 n...
Journal Articles
Alloy Digest (1994) 43 (12): Ni-473.
Published: 01 December 1994
...: Nickel Alloy Ni-473 DECEMBER 1994 DATA ON WORLD WIDE METALS AND ALLOYS Phtshdby: Alg Di@W. Inc IZQ1677-6161 NICORROS = AL 27 Canliild SImeI. Or;moe. NJ. 07050 I U.S.A. (Age-hardenable nlokel-copper alloy) NICORROS AL is age-hardenable by virtue of the alloying additions of aluminum and titanium...
Journal Articles
Alloy Digest (1996) 45 (11): SS-660.
Published: 01 November 1996
... CLI-50A is a Korean 6 Mo superaustenitic stainless steel with improved corrosion resistance properties. The chromium additions have been increased up to 22% together with high nitrogen additions. The PREN value [%Cr] + 3.3 [%Mo] + 16[%N] is higher than 45. The alloy is copper free. This alloy...