Alloy Digest (1966) 15 (9): Cu-168.
Published: 01 September 1966
... Copper Alloy 720 is a copper-nickel alloy having high corrosion resistance and retention of strength at moderately elevated temperatures. It is recommended for heat exchangers, salt water piping and relays. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1964) 13 (7): Cu-143.
Published: 01 July 1964
... CONFLEX 720 is a copper-manganese-nickel alloy that responds to an age-hardening heat treatment for high strength and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on...
Journal Articles
Alloy Digest (1954) 3 (1): Cu-14.
Published: 01 January 1954
... C.D.C. MANGANESE ALLOY No. 720 is a copper-manganese-nickel alloy that responds to hardening by heat treatment. It has high tensile and fatigue strength, wide hardness range, and excellent corrosion resisting characteristics. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2004) 53 (8): Cu-720.
Published: 01 August 2004
... conductivity are needed at higher temperatures than most connector alloys can retain. Producer: Olin Brass East Alton, IL 62024-1197 (618) 258-5255 (618) 258-2769 (fax) e-mail: Info@olinbrass.com Web: www.olinbrass.com ISSN: 002-614X OLIN ALLOY C4252 Filing Code: Cu-720 Copper August 2004 OLIN ALLOY C4252 (Tin...
Journal Articles
Alloy Digest (2015) 64 (2): Ni-720.
Published: 01 February 2015
... NSSMC 696 is a high-temperature alloy with noted resistance to metal dusting. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Ni-720. Producer...
Journal Articles
Alloy Digest (2004) 53 (3): Cu-712.
Published: 01 March 2004
..., making it possible to produce an alloy that has both high strength and high conductivity. Alloy 390 combines the best attributes of two separate families of commercial copper-beryllium alloys: the strength of the high-strength alloy C17200 with the conductivity of high-conductivity alloys C17410 and...
Journal Articles
Alloy Digest (1992) 41 (8): Cu-575.
Published: 01 August 1992
... BRUSH CASTING ALLOY 21C is a beryllium copper alloy of high strength with cobalt as the second alloying element (1.0 to 2.0% Co). Use is in age-hardened temper. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1992) 41 (9): Cu-576.
Published: 01 September 1992
... BRUSH CASTING ALLOYS 165C AND 165CT are beryllium copper alloys of high strength with cobalt as the second alloying element (0.20 to 0.65% Co). Use is in the age-hardened temper. Brush casting alloy 165CT is the fine-grained version. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1992) 41 (10): Cu-577.
Published: 01 October 1992
... BRUSH CASTING ALLOYS 245C AND 245CT are beryllium copper (2.25-2.55% Be) alloys of high strength with cobalt as the second alloying element (0.35-0.70% Co). Use is in the age-hardened temper. Brush casting alloy 245CT is the fine-grained version. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1993) 42 (1): Cu-581.
Published: 01 January 1993
... BRUSH CASTING ALLOYS 20C AND 20CT are beryllium copper alloys (1.90-2.15% Be) of very high strength with cobalt as the second alloying element (0.35 to 0.70% Co). Use is in the age-hardened temper. Brush casting alloy 20CT is the fine-grained version. This datasheet provides information on...
Journal Articles
Alloy Digest (1992) 41 (12): Cu-537.
Published: 01 December 1992
... BRUSH CASTING ALLOYS 275C AND 275CT are beryllium copper alloys of very high strength with cobalt and silicon as the secondary alloying elements. Use is in the age-hardened temper. Brush casting alloy 275CT is the fine-grained version. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2004) 53 (6): Cu-717.
Published: 01 June 2004
... Brush 60 is a high-performance, lower-priced copper beryllium alloy offering cost-effective solutions for many applications such as electronic contacts and springs in the computer, datacom, and telecommunications markets. It is available in mill-hardened tempers. This datasheet provides...
Journal Articles
Alloy Digest (2018) 67 (6): Cu-873.
Published: 01 June 2018
... Alloy CuSn6 (UNS C51900) is a high-performance copper alloy. Typical uses include components for the electronics industry such as connector springs, relays, leaf springs, and switches as well as machine parts. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2018) 67 (8): Cu-877.
Published: 01 August 2018
... Alloy CuSn10 is a high-performance copper alloy. The alloy is characterized by good electrical and thermal conductivity and very good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength...
Journal Articles
Alloy Digest (2019) 68 (1): Cu-883.
Published: 01 January 2019
... Alloy 7026 is a copper-nickel-silicon alloy for the electrical industry. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on corrosion resistance. Filing Code: Cu-883. Producer or source: Gebr...
Journal Articles
Alloy Digest (2005) 54 (9): Cu-736.
Published: 01 September 2005
... Marinel 220 is a copper alloy of 18% Ni with high manganese and aluminum. It develops high strength with excellent corrosion resistance. It is the successor alloy to Marinel (see Alloy Digest Cu-602, December 1995). This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2018) 67 (5): Cu-871.
Published: 01 May 2018
... Alloy CuSn5 (UNS C51000) is a high-performance copper alloy. The alloy is characterized by good tensile strength, good electrical conductivity, and very good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (2020) 69 (3): Cu-906.
Published: 01 March 2020
... Wieland Duro Elmedur HA is a heat-treatable copper-cobalt-nickel-beryllium alloy. In the age hardened condition, this alloy exhibits high electrical and thermal conductivity along with moderate strength and hardness. This datasheet provides information on composition, physical properties, and...
Journal Articles
Alloy Digest (2013) 62 (11): Cu-826.
Published: 01 November 2013
... MoldMAX XL is a high-strength copper mold alloy with good conductivity. The alloy contains no beryllium and is available in sections as large as 305 mm (12 in.) thick. The alloy’s hardness is comparable to AISI P-20 tool steel, but its thermal conductivity is two to three times higher. This alloy...
Journal Articles
Alloy Digest (1984) 33 (5): Ni-297.
Published: 01 May 1984
.... Composition: (Weight %) Nominal Nickel 42 Chromium 21 Molybdenum 3 Copper 2.2 Titanium 2. I Aluminum 0.3 Carbon 0.02 iron 32 Table 1 - SPECIFIC HEAT Physical Constants: Density, Ib!cu in. (At 7O F) 0.294 g;cu cm (At 21°C) 8. 14 Melting range. F(OC) 2392-2490 ( I3 I I- 1366) Specific heat & Thermal expansion...