Alloy Digest (1954) 3 (11): SS-20.
Published: 01 November 1954
... COOPER ALLOY V2B is a precipitation-hardening, wear and corrosion resisting stainless steel of the 18-8 type. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, joining...